Dislocation creep behavior in Mg–Al–Zn alloys H Somekawa, K Hirai, H Watanabe, Y Takigawa, K Higashi Materials Science and Engineering: A 407 (1-2), 53-61, 2005 | 338 | 2005 |
Effects of Ca and Sr addition on mechanical properties of a cast AZ91 magnesium alloy at room and elevated temperature K Hirai, H Somekawa, Y Takigawa, K Higashi Materials Science and Engineering: A 403 (1-2), 276-280, 2005 | 336 | 2005 |
Compressive response of a closed-cell aluminum foam at high strain rate T Mukai, T Miyoshi, S Nakano, H Somekawa, K Higashi Scripta Materialia 54 (4), 533-537, 2006 | 223 | 2006 |
Effect of grain refinement on fracture toughness in extruded pure magnesium H Somekawa, T Mukai Scripta materialia 53 (9), 1059-1064, 2005 | 210 | 2005 |
Transition of dominant deformation mode in bulk polycrystalline pure Mg by ultra-grain refinement down to sub-micrometer R Zheng, JP Du, S Gao, H Somekawa, S Ogata, N Tsuji Acta Materialia 198, 35-46, 2020 | 193 | 2020 |
Effect of texture on fracture toughness in extruded AZ31 magnesium alloy H Somekawa, T Mukai Scripta materialia 53 (5), 541-545, 2005 | 162 | 2005 |
Low temperature diffusion bonding in a superplastic AZ31 magnesium alloy H Somekawa, H Watanabe, T Mukai, K Higashi Scripta Materialia 48 (9), 1249-1254, 2003 | 150 | 2003 |
Effect of solid solution elements on nanoindentation hardness, rate dependence, and incipient plasticity in fine grained magnesium alloys H Somekawa, CA Schuh Acta materialia 59 (20), 7554-7563, 2011 | 148 | 2011 |
Diffusion bonding in superplastic magnesium alloys H Somekawa, H Hosokawa, H Watanabe, K Higashi Materials Science and Engineering: A 339 (1-2), 328-333, 2003 | 147 | 2003 |
Fracture mechanism of a coarse-grained magnesium alloy during fracture toughness testing H Somekawa, A Singh, T Mukai Philosophical Magazine Letters 89 (1), 2-10, 2009 | 146 | 2009 |
Precipitation control of calcium phosphate on pure magnesium by anodization S Hiromoto, T Shishido, A Yamamoto, N Maruyama, H Somekawa, ... Corrosion Science 50 (10), 2906-2913, 2008 | 140 | 2008 |
High strength and fracture toughness balance on the extruded Mg–Ca–Zn alloy H Somekawa, T Mukai Materials Science and Engineering: A 459 (1-2), 366-370, 2007 | 139 | 2007 |
Effect of texture on tensile properties at elevated temperatures in an AZ31 magnesium alloy H Watanabe, A Takara, H Somekawa, T Mukai, K Higashi Scripta Materialia 52 (6), 449-454, 2005 | 130 | 2005 |
Hall–Petch relation for deformation twinning in solid solution magnesium alloys H Somekawa, T Mukai Materials Science and Engineering: A 561, 378-385, 2013 | 128 | 2013 |
Compressive strength and yield asymmetry in extruded Mg–Zn–Ho alloys containing quasicrystal phase A Singh, H Somekawa, T Mukai Scripta Materialia 56 (11), 935-938, 2007 | 123 | 2007 |
Ultra-fine grain size and isotropic very high strength by direct extrusion of chill-cast Mg–Zn–Y alloys containing quasicrystal phase A Singh, Y Osawa, H Somekawa, T Mukai Scripta Materialia 64 (7), 661-664, 2011 | 121 | 2011 |
High fracture toughness of extruded Mg–Zn–Y alloy by the synergistic effect of grain refinement and dispersion of quasicrystalline phase H Somekawa, A Singh, T Mukai Scripta Materialia 56 (12), 1091-1094, 2007 | 121 | 2007 |
Hall–Petch breakdown in fine-grained pure magnesium at low strain rates H Somekawa, T Mukai Metallurgical and Materials Transactions A 46, 894-902, 2015 | 112 | 2015 |
Fracture toughness in Mg–Al–Zn alloy processed by equal-channel-angular extrusion H Somekawa, T Mukai Scripta materialia 54 (4), 633-638, 2006 | 104 | 2006 |
Effect of solid-solution strengthening on fracture toughness in extruded Mg–Zn alloys H Somekawa, Y Osawa, T Mukai Scripta materialia 55 (7), 593-596, 2006 | 95 | 2006 |