Mechanisms of sliding wear of metals and alloys at elevated temperatures
A Pauschitz, M Roy, F Franek
Tribology International 41 (7), 584-602, 2008
3222008
Microstructure and mechanical properties of HVOF sprayed nanocrystalline Cr3C2-25(Ni20Cr) coating
M Roy, A Pauschitz, J Bernardi, T Koch, F Franek
Journal of thermal spray technology 15, 372-381, 2006
832006
Comparative evaluation of ambient temperature friction behaviour of thermal sprayed Cr3C2–25 (Ni20Cr) coatings with conventional and nano-crystalline grains
M Roy, A Pauschitz, R Polak, F Franek
Tribology International 39 (1), 29-38, 2006
632006
The influence of temperature on the wear of Cr3C2–25 (Ni20Cr) coating—comparison between nanocrystalline grains and conventional grains
M Roy, A Pauschitz, J Wernisch, F Franek
Wear 257 (7-8), 799-811, 2004
542004
Nanotribological simulations of multi-grit polishing and grinding
SJ Eder, U Cihak-Bayr, A Pauschitz
Wear 340, 25-30, 2015
462015
Micro-and nanomechanical properties of diamond film with various surface morphologies
A Bogus, IC Gebeshuber, A Pauschitz, M Roy, R Haubner
Diamond and Related Materials 17 (12), 1998-2004, 2008
432008
Nanoindentation and nanoscratch behaviour of reactive sputtered deposited W–S–C film
T Koch, M Evaristo, A Pauschitz, M Roy, A Cavaleiro
Thin Solid Films 518 (1), 185-193, 2009
412009
Nanotribological study of PECVD DLC and reactively sputtered Ti containing carbon films
S Kvasnica, J Schalko, C Eisenmenger-Sittner, J Benardi, G Vorlaufer, ...
Diamond and related materials 15 (10), 1743-1752, 2006
382006
Effect of mating surface on the high temperature wear of 253 MA alloy
M Roy, A Pauschitz, J Wernisch, F Franek
Materials and Corrosion 55 (4), 259-273, 2004
312004
Nanoindentation and AFM studies of PECVD DLC and reactively sputtered Ti containing carbon films
A Pauschitz, J Schalko, T Koch, C Eisenmenger-Sittner, S Kvasnica, ...
Bulletin of Materials Science 26, 585-591, 2003
312003
Gelatin methacryloyl as environment for chondrocytes and cell delivery to superficial cartilage defects
K Hölzl, M Fürsatz, H Göcerler, B Schädl, S Žigon‐Branc, M Markovic, ...
Journal of tissue engineering and regenerative medicine 16 (2), 207-222, 2022
302022
Combined experimental and numerical simulation of abrasive wear and its application to a tillage machine component
PO Bedolla, G Vorlaufer, C Rechberger, D Bianchi, SJ Eder, R Polak, ...
Tribology International 127, 122-128, 2018
302018
Tribological investigation of nanocrystalline diamond films at low load under different tribosystems
M Roy, S Ghodbane, T Koch, A Pauschitz, D Steinmüller–Nethl, A Tomala, ...
Diamond and related materials 20 (4), 573-583, 2011
272011
Tribological behaviour of Ti containing nanocomposite DLC films under milli-Newton load range
A Pauschitz, S Kvasnica, R Jisa, J Bernardi, T Koch, M Roy
Diamond and related materials 17 (12), 2010-2018, 2008
232008
Experimental investigation on wear map evolution of ceramic-on-UHMWPE hip prosthesis
L Mattei, F Di Puccio, E Ciulli, A Pauschitz
Tribology International 143, 106068, 2020
222020
Nanotribology of pulsed direct current magnetron sputtered diamond like carbon films
A Tomala, A Pauschitz, M Roy
Surface science 616, 60-70, 2013
202013
The influence of sputtering procedure on nanoindentation and nanoscratch behaviour of W–S–C film
M Roy, T Koch, A Pauschitz
Applied surface science 256 (22), 6850-6858, 2010
182010
Evaluation of ionic liquids as lubricants
N Dörr, IC Gebeshuber, D Holzer, HD Wanzenböck, A Ecker, A Pauschitz, ...
na, 2010
172010
On the scratch behaviour of self-lubricating WSe2 films
A Pauschitz, E Badisch, M Roy, DV Shtansky
Wear 267 (11), 1909-1914, 2009
172009
Friction and wear measurements of laser-sintered and coated parts
J Takacs, L Tóth, F Franek, A Pauschitz, T Sebestyén
Wear 256 (11-12), 1228-1231, 2004