Effect of grain size on friction and wear of nanocrystalline aluminum ZN Farhat, Y Ding, DO Northwood, AT Alpas Materials Science and Engineering: A 206 (2), 302-313, 1996 | 305 | 1996 |
Effect of impact angle and velocity on erosion of API X42 pipeline steel under high abrasive feed rate MA Islam, ZN Farhat Wear 311 (1-2), 180-190, 2014 | 200 | 2014 |
Early failure of a modular femoral neck total hip arthroplasty component: a case report DAJ Wilson, MJ Dunbar, JD Amirault, Z Farhat JBJS 92 (6), 1514-1517, 2010 | 123 | 2010 |
Recent advances in electroless-plated Ni-P and its composites for erosion and corrosion applications: a review EM Fayyad, AM Abdullah, MK Hassan, AM Mohamed, G Jarjoura, ... Emergent Materials 1, 3-24, 2018 | 113 | 2018 |
Erosion enhanced corrosion and corrosion enhanced erosion of API X-70 pipeline steel MA Islam, ZN Farhat, EM Ahmed, AM Alfantazi Wear 302 (1-2), 1592-1601, 2013 | 112 | 2013 |
Wear mechanism of CBN cutting tool during high-speed machining of mold steel ZN Farhat Materials Science and Engineering: A 361 (1-2), 100-110, 2003 | 105 | 2003 |
Sliding wear of superelastic TiNi alloy C Zhang, ZN Farhat Wear 267 (1-4), 394-400, 2009 | 96 | 2009 |
Erosion-corrosion mechanism and comparison of erosion-corrosion performance of API steels MA Islam, Z Farhat Wear 376, 533-541, 2017 | 95 | 2017 |
Nanoindentation and friction studies on Ti-based nanolaminated films ZN Farhat, Y Ding, DO Northwood, AT Alpas Surface and Coatings Technology 89 (1-2), 24-30, 1997 | 81 | 1997 |
Indentation and erosion behavior of electroless Ni-P coating on pipeline steel C Wang, Z Farhat, G Jarjoura, MK Hassan, AM Abdullah Wear 376, 1630-1639, 2017 | 80 | 2017 |
Effect of microstructure on the erosion behavior of carbon steel MA Islam, T Alam, ZN Farhat, A Mohamed, A Alfantazi Wear 332, 1080-1089, 2015 | 78 | 2015 |
The synergistic effect between erosion and corrosion of API pipeline in CO2 and saline medium MA Islam, ZN Farhat Tribology International 68, 26-34, 2013 | 74 | 2013 |
Modeling of catalyst layer microstructural refinement and catalyst utilization in a PEM fuel cell ZN Farhat Journal of Power Sources 138 (1-2), 68-78, 2004 | 66 | 2004 |
Slurry erosion of pipeline steel: effect of velocity and microstructure T Alam, M Aminul Islam, ZN Farhat Journal of Tribology 138 (2), 021604, 2016 | 64 | 2016 |
Contribution of crystallographic texturing to the sliding friction behaviour of fcc and hcp metals ZN Farhat Wear 250 (1-12), 401-408, 2001 | 64 | 2001 |
Wear and dent resistance of superelastic TiNi alloy R Neupane, Z Farhat Wear 301 (1-2), 682-687, 2013 | 59 | 2013 |
Reciprocating wear behaviour of TiC-stainless steel cermets C Jin, CC Onuoha, ZN Farhat, GJ Kipouros, KP Plucknett Tribology International 105, 250-263, 2017 | 58 | 2017 |
The reciprocating wear behaviour of TiC–304L stainless steel composites prepared by melt infiltration CC Onuoha, GJ Kipouros, ZN Farhat, KP Plucknett Wear 303 (1-2), 321-333, 2013 | 56 | 2013 |
Effect of porosity on dry sliding wear of Al–Si alloys MA Islam, ZN Farhat Tribology International 44 (4), 498-504, 2011 | 55 | 2011 |
The influence of porosity and hot isostatic pressing treatment on wear characteristics of cast and P/M aluminum alloys MA Islam, ZN Farhat Wear 271 (9-10), 1594-1601, 2011 | 54 | 2011 |