Computer analysis of characteristic elements of fractographic images
RY Kosarevych, OZ Student, LM Svirs’ ka, BP Rusyn, HM Nykyforchyn
Materials Science 48, 474-481, 2013
612013
Evaluation of the influence of shutdowns of a technological process on changes in the in-service state of the metal of main steam pipelines of thermal power plants
HM Nykyforchyn, OZ Student, HV Krechkovs’ ka, AD Markov
Materials Science 46, 177-189, 2010
492010
Accelerated method for hydrogen degradation of structural steel
OZ Student
Materials Science 34 (4), 497-507, 1998
491998
Arc-sprayed iron-based coatings for erosion-corrosion protection of boiler tubes at elevated temperatures
V Pokhmurskii, M Student, V Gvozdeckii, T Stypnutskyy, O Student, ...
Journal of thermal spray technology 22, 808-819, 2013
472013
Abnormal manifestation of the high-temperature degradation of the weld metal of a low-alloy steel welded joint
HM Nykyforchyn, OZ Student, AD Markov
Materials Science 43, 77-84, 2007
472007
The properties of oxide-ceramic layers with Cu and Ni inclusions synthesizing by PEO method on top of the gas-spraying coatings on aluminium alloys
V Hutsaylyuk, M Student, V Posuvailo, O Student, Y Sirak, V Hvozdets' kyi, ...
Vacuum 179, 109514, 2020
362020
Features of the microstructural and mechanical degradation of long term operated mild steel
H Krechkovska, O Student, G Lesiuk, J Correia
International Journal of Structural Integrity 9 (3), 296-306, 2018
332018
Assessment of operational degradation of pipeline steels
H Nykyforchyn, O Zvirko, I Dzioba, H Krechkovska, M Hredil, O Tsyrulnyk, ...
Materials 14 (12), 3247, 2021
292021
Study of the fatigue crack growth in long-term operated mild steel under mixed-mode (I+ II, I+ III) loading conditions
G Lesiuk, M Smolnicki, D Rozumek, H Krechkovska, O Student, J Correia, ...
Materials 13 (1), 160, 2020
272020
Feature of stress corrosion cracking of degraded gas pipeline steels
H Nykyforchyn, H Krechkovska, O Student, O Zvirko
Procedia Structural Integrity 16, 153-160, 2019
262019
Effect of hydrogen on the wear resistance of steels upon contact with plasma electrolytic oxidation layers synthesized on aluminum alloys
V Hutsaylyuk, M Student, V Dovhunyk, V Posuvailo, O Student, ...
Metals 9 (3), 280, 2019
242019
Determination of the degree of degradation of steels of steam pipelines according to their impact toughness on specimens with different geometries of notches
HV Krechkovs’ ka, OZ Student
Materials Science 52, 566-571, 2017
242017
Improvement of wear resistance of aluminum alloy by HVOF method
V Hutsaylyuk, M Student, K Zadorozhna, O Student, H Veselivska, ...
Journal of Materials Research and Technology 9 (6), 16367-16377, 2020
232020
Anisotropy of the mechanical properties of degraded 15Kh1М1F steel after its operation in steam pipelines of thermal power plants
ОZ Student, HV Krechkovs’ ka
Materials Science 47, 590-597, 2012
232012
Аномальний прояв високотемпературної деградації металу шва зварного з’єднання ощаднолегованої сталі
ГМ Никифорчин, ОЗ Студент, АД Марков
Фіз.-хім. механіка матеріалів 43 (1), 73-79, 2007
232007
Influence of the long-term operation of 12Kh1M1F steel from different zones of a bend of steam pipeline of a thermal power plant on its mechanical characteristics
OZ Student, LM Svirs’ ka, IR Dzioba
Materials Science 48, 239-246, 2012
222012
Effect of high-force impulse loads on the modification of mechanical properties of heat-resistant steel after service
M Chausov, P Maruschak, A Pylypenko, F Sergejev, O Student
Estonian Journal of Engineering 18 (3), 251, 2012
222012
In-service degradation of mechanical characteristics of pipe steels in gas mains
HV Krechkovs’ ka, OT Tsyrul’nyk, OZ Student
Strength of Materials 51, 406-417, 2019
212019
Fractographic features of long term operated gas pipeline steels fracture under impact loading
M Hredil, H Krechkovska, O Student, I Kurnat
Procedia Structural Integrity 21, 166-172, 2019
212019
Degradation of welded joints of steam pipelines of thermal electric power plants in hydrogenating media
HM Nykyforchyn, OZ Student, IR Dzioba, SM Stepanyuk, AD Markov, ...
Materials Science 40, 836-843, 2004