Korozija i zaštita premazima I Juraga, V Alar, I Stojanović | 133 | 2014 |
Synergistic inhibition of carbon steel corrosion in seawater by cerium chloride and sodium gluconate F Ivušić, O Lahodny-Šarc, HO Ćurković, V Alar Corrosion science 98, 88-97, 2015 | 94 | 2015 |
Kemijska postojanost metala V Alar | 55 | 2015 |
Mehanizmi zaštite od korozije, autorizirana predavanja I Juraga, V Šimunović, I Stojanović, V Alar Fakultet strojarstva i brodogradnje, Zagreb, 2012 | 44 | 2012 |
Influence of thermal oxides on pitting corrosion of stainless steel in chloride solutions I Esih, V Alar, I Juraga Corrosion engineering, science and technology 40 (2), 110-120, 2005 | 31 | 2005 |
Experimental evaluation of polyester and epoxy–polyester powder coatings in aggressive media I Stojanović, V Šimunović, V Alar, F Kapor Coatings 8 (3), 98, 2018 | 28 | 2018 |
Corrosion inhibition of carbon steel in various water types by zinc gluconate F Ivušić, O Lahodny‐Šarc, V Alar Materialwissenschaft und Werkstofftechnik 44 (4), 319-329, 2013 | 24 | 2013 |
Korozija i metode zaštite od korozije, skripta I Juraga, V Alar, I Stojanović, V Šimunović Fakultet strojarstva i brodogradnje, Zagreb, 2011 | 23 | 2011 |
Development of models for prediction of corrosion and pitting potential on AISI 304 stainless steel in different environmental conditions V Alar, I Žmak, B Runje, A Horvatić International Journal of electrochemical science 11 (9), 7674-7689, 2016 | 22 | 2016 |
Teorijske osnove korozijskih procesa i metode zaštite V Alar, V Šimunović, I Juraga Autorizirana predavanja. Zagreb, 2011 | 22 | 2011 |
Electrochemical Behaviour of PACVD TiN-Coated CoCrMo Medical Alloy S Jakovljević, V Alar, A Ivanković Metals 7 (7), 231, 2017 | 16 | 2017 |
Electrochemical corrosion behavior of near-nano and nanostructured WC-Co cemented carbides Ž Alar, V Alar, TA Fabijanić Metals 7 (3), 69, 2017 | 16 | 2017 |
Corrosion properties of thermal sprayed aluminium (TSA) coatings deposited by powder flame spraying Z Glogović, V Alar, Z Kožuh, I Stojanović, S Kralj Materialwissenschaft und Werkstofftechnik 42 (3), 224-228, 2011 | 14 | 2011 |
Evaluation of the corrosion protection of two underwater coating systems in a simulated marine environment I Stojanović, A Farkas, V Alar, N Degiuli JOM 71 (12), 4330-4338, 2019 | 13 | 2019 |
Effect of the cerium (III) chloride heptahydrate on the corrosion inhibition of aluminum alloy M Kurtela, V Šimunović, I Stojanović, V Alar Materials and Corrosion 71 (1), 125-147, 2020 | 12 | 2020 |
Corrosion Resistance of Highly Alloyed Materials in 3.5% NaCl solution at elevated temperature V Alar, I Stojanović, B Židov, F Ivušić International journal of electrochemical science 8 (12), 12476-12486, 2013 | 12 | 2013 |
A significant improvement in material of foam A Đukić, V Alar, M Firak, S Jakovljević Journal of alloys and compounds 573, 128-132, 2013 | 12 | 2013 |
Zaštita ugljičnog čelika vodorazrjedivim premazima V Alar, I Stojanović, I Mihalic Zaštita materijala 52 (3), 201-203, 2011 | 12 | 2011 |
Corrosion behaviour of an epoxy resin reinforced with aluminium nanoparticles M Samardžija, V Alar, V Špada, I Stojanović Coatings 12 (10), 1500, 2022 | 11 | 2022 |
The effect of temperature on corrosion behavior of AA5083 in brackish water and seawater L Lokas, V Alar Materials and corrosion 70 (10), 1817-1825, 2019 | 11 | 2019 |