SFPE handbook of fire protection engineering MJ Hurley, DT Gottuk, JR Hall Jr, K Harada, ED Kuligowski, M Puchovsky, ... Springer, 2015 | 1834 | 2015 |
Development of fire‐retarded materials—interpretation of cone calorimeter data B Schartel, TR Hull Fire and Materials: An International Journal 31 (5), 327-354, 2007 | 1502 | 2007 |
Flammability behaviour of wood and a review of the methods for its reduction LA Lowden, TR Hull Fire science reviews 2, 1-19, 2013 | 470 | 2013 |
Fire retardant action of mineral fillers TR Hull, A Witkowski, L Hollingbery Polymer degradation and stability 96 (8), 1462-1469, 2011 | 421 | 2011 |
Mechanism of thermal decomposition of poly (ether ether ketone)(PEEK) from a review of decomposition studies P Patel, TR Hull, RW McCabe, D Flath, J Grasmeder, M Percy Polymer degradation and stability 95 (5), 709-718, 2010 | 397 | 2010 |
Assessment of the fire toxicity of building insulation materials AA Stec, TR Hull Energy and Buildings 43 (2-3), 498-506, 2011 | 298 | 2011 |
The thermal decomposition of huntite and hydromagnesite—a review LA Hollingbery, TR Hull Thermochimica Acta 509 (1-2), 1-11, 2010 | 297 | 2010 |
Fire retardancy of a reactively extruded intumescent flame retardant polyethylene system enhanced by metal chelates DY Wang, Y Liu, YZ Wang, CP Artiles, TR Hull, D Price Polymer Degradation and Stability 92 (8), 1592-1598, 2007 | 207 | 2007 |
The fire retardant behaviour of huntite and hydromagnesite–A review LA Hollingbery, TR Hull Polymer degradation and stability 95 (12), 2213-2225, 2010 | 197 | 2010 |
Flame retardance of poly (methyl methacrylate) modified with phosphorus-containing compounds D Price, K Pyrah, TR Hull, GJ Milnes, JR Ebdon, BJ Hunt, P Joseph Polymer Degradation and Stability 77 (2), 227-233, 2002 | 191 | 2002 |
The fire toxicity of polyurethane foams ST McKenna, TR Hull Fire Science Reviews 5, 1-27, 2016 | 184 | 2016 |
Fire behaviour of modern façade materials–Understanding the Grenfell Tower fire ST McKenna, N Jones, G Peck, K Dickens, W Pawelec, S Oradei, S Harris, ... Journal of hazardous materials 368, 115-123, 2019 | 174 | 2019 |
Fire toxicity AA Stec, TR Hull Elsevier, 2010 | 164 | 2010 |
Fire retardancy of polymers: new strategies and mechanisms N Cinausero, B Howell, G Schmaucks, G Marosi, Z Brzozwski, JM Cuesta, ... The Royal Society of Chemistry, 2008 | 163 | 2008 |
Synthesis of mesoporous silica@ Co–Al layered double hydroxide spheres: layer-by-layer method and their effects on the flame retardancy of epoxy resins SD Jiang, ZM Bai, G Tang, L Song, AA Stec, TR Hull, Y Hu, WZ Hu ACS applied materials & interfaces 6 (16), 14076-14086, 2014 | 160 | 2014 |
Investigation of the thermal decomposition and flammability of PEEK and its carbon and glass-fibre composites P Patel, TR Hull, RE Lyon, SI Stoliarov, RN Walters, S Crowley, ... Polymer degradation and stability 96 (1), 12-22, 2011 | 148 | 2011 |
An investigation into the decomposition and burning behaviour of Ethylene-vinyl acetate copolymer nanocomposite materials TR Hull, D Price, Y Liu, CL Wills, J Brady Polymer Degradation and Stability 82 (2), 365-371, 2003 | 147 | 2003 |
Fire Retardancy of Polymers PR Hornsby, RN Rothon, K Takeda, C Pelegris, T Kashiwagi, S Lomakin, ... The Royal Society of Chemistry, 2005 | 146 | 2005 |
Thermal decomposition of polymeric materials A Witkowski, AA Stec, TR Hull SFPE handbook of fire protection engineering, 167-254, 2016 | 137 | 2016 |
Thermal behaviour of covalently bonded phosphate and phosphonate flame retardant polystyrene systems D Price, LK Cunliffe, KJ Bullett, TR Hull, GJ Milnes, JR Ebdon, BJ Hunt, ... Polymer Degradation and Stability 92 (6), 1101-1114, 2007 | 131 | 2007 |