Ceramic matrix composites: materials, modeling and technology NP Bansal, J Lamon John Wiley & Sons, 2014 | 316 | 2014 |
The tensile behavior of carbon fibers at high temperatures up to 2400 C C Sauder, J Lamon, R Pailler Carbon 42 (4), 715-725, 2004 | 249 | 2004 |
Damage and failure in ceramic matrix minicomposites: experimental study and model N Lissart, J Lamon Acta Materialia 45 (3), 1025-1044, 1997 | 220 | 1997 |
A micromechanics-based approach to the mechanical behavior of brittle-matrix composites J Lamon Composites science and technology 61 (15), 2259-2272, 2001 | 217 | 2001 |
Fracture toughness of 2‐D woven SiC/SiC CVI‐composites with multilayered interphases C Droillard, J Lamon Journal of the American Ceramic Society 79 (4), 849-858, 1996 | 207 | 1996 |
Single‐and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: an overview RR Naslain, RJF Pailler, JL Lamon International Journal of Applied Ceramic Technology 7 (3), 263-275, 2010 | 180 | 2010 |
The concept of a strong interface applied to SiC/SiC composites with a BN interphase F Rebillat, J Lamon, A Guette Acta materialia 48 (18-19), 4609-4618, 2000 | 164 | 2000 |
Microcomposite test procedure for evaluating the interface properties of ceramic matrix composites J Lamon, F Rebillat, AG Evans Journal of the American Ceramic Society 78 (2), 401-405, 1995 | 152 | 1995 |
Thermomechanical properties of carbon fibres at high temperatures (up to 2000 C) C Sauder, J Lamon, R Pailler Composites Science and Technology 62 (4), 499-504, 2002 | 147 | 2002 |
Statistical analysis of bending strengths for brittle solids: a multiaxial fracture problem J Lamon, AG EVANS Journal of the American Ceramic Society 66 (3), 177-182, 1983 | 145 | 1983 |
Tensile creep behaviour of a silicon carbide-based fibre with a low oxygen content R Bodet, X Bourrat, J Lamon, R Naslain Journal of materials science 30, 661-677, 1995 | 143 | 1995 |
Statistical approaches to failure for ceramic reliability assessment J Lamon Journal of the American Ceramic Society 71 (2), 106-112, 1988 | 135 | 1988 |
The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites N Carrère, E Martin, J Lamon Composites Part A: Applied Science and Manufacturing 31 (11), 1179-1190, 2000 | 130 | 2000 |
Micro/minicomposites: a useful approach to the design and development of non-oxide CMCs R Naslain, J Lamon, R Pailler, X Bourrat, A Guette, F Langlais Composites Part A: applied science and manufacturing 30 (4), 537-547, 1999 | 130 | 1999 |
Influence of interface characteristics on the mechanical properties of Hi‐Nicalon type‐S or Tyranno‐SA3 fiber‐reinforced SiC/SiC minicomposites C Sauder, A Brusson, J Lamon International Journal of Applied Ceramic Technology 7 (3), 291-303, 2010 | 122 | 2010 |
Properties of multilayered interphases in SiC/SiC chemical‐vapor‐infiltrated composites with “weak” and “strong” interfaces F Rebillat, J Lamon, R Naslain, E Lara‐Curzio, MK Ferber, TM Besmann Journal of the American Ceramic Society 81 (9), 2315-2326, 1998 | 120 | 1998 |
Failure of fiber bundles V Calard, J Lamon Composites science and technology 64 (5), 701-710, 2004 | 117 | 2004 |
Hi‐Nicalon/SiC Minicomposites with (Pyrocarbon/SiC)n Nanoscale Multilayered Interphases S Bertrand, P Forio, R Pailler, J Lamon Journal Of The American Ceramic Society 82 (9), 2465-2473, 1999 | 115 | 1999 |
Sliding friction of ceramics: mechanical action of the wear debris J Denape, J Lamon Journal of materials science 25, 3592-3604, 1990 | 112 | 1990 |
Delayed failure of Hi‐Nicalon and Hi‐Nicalon S multifilament tows and single filaments at intermediate temperatures (500–800 C) W Gauthier, J Lamon Journal of the American Ceramic Society 92 (3), 702-709, 2009 | 110 | 2009 |