关注
Kim Vanmeensel
Kim Vanmeensel
Associate Professor, Department of Materials Engineering, KU Leuven
在 kuleuven.be 的电子邮件经过验证 - 首页
标题
引用次数
引用次数
年份
Modelling of the temperature distribution during field assisted sintering
K Vanmeensel, A Laptev, J Hennicke, J Vleugels, O Van der Biest
Acta Materialia 53 (16), 4379-4388, 2005
5672005
Influence of selective laser melting process parameters on texture evolution in pure copper
SD Jadhav, S Dadbakhsh, L Goossens, JP Kruth, J Van Humbeeck, ...
Journal of Materials Processing Technology 270, 47-58, 2019
2582019
Selective laser melting of tungsten and tungsten alloys
A Iveković, N Omidvari, B Vrancken, K Lietaert, L Thijs, K Vanmeensel, ...
International Journal of Refractory Metals and Hard Materials 72, 27-32, 2018
2342018
Microstructure evolution of 316L produced by HP-SLM (high power selective laser melting)
ML Montero-Sistiaga, M Godino-Martinez, K Boschmans, JP Kruth, ...
Additive Manufacturing 23, 402-410, 2018
2312018
Laser powder bed fusion of Hastelloy X: Effects of hot isostatic pressing and the hot cracking mechanism
Q Han, R Mertens, ML Montero-Sistiaga, S Yang, R Setchi, K Vanmeensel, ...
Materials Science and Engineering: A 732, 228-239, 2018
2052018
Influence of sintering conditions on low-temperature degradation of dental zirconia
M Inokoshi, F Zhang, J De Munck, S Minakuchi, I Naert, J Vleugels, ...
Dental materials 30 (6), 669-678, 2014
1922014
Highly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation
F Zhang, K Vanmeensel, M Batuk, J Hadermann, M Inokoshi, ...
Acta biomaterialia 16, 215-222, 2015
1862015
Microstructure and mechanical properties of Hastelloy X produced by HP-SLM (high power selective laser melting)
ML Montero-Sistiaga, S Pourbabak, J Van Humbeeck, D Schryvers, ...
Materials & Design 165, 107598, 2019
1762019
Effect of post-treatments on the fatigue behaviour of 316L stainless steel manufactured by laser powder bed fusion
C Elangeswaran, A Cutolo, GK Muralidharan, C de Formanoir, F Berto, ...
International Journal of Fatigue 123, 31-39, 2019
1632019
Aging resistance of surface-treated dental zirconia
M Inokoshi, K Vanmeensel, F Zhang, J De Munck, G Eliades, S Minakuchi, ...
Dental Materials 31 (2), 182-194, 2015
1602015
Microstructure and mechanical properties of pulsed electric current sintered B4C–TiB2 composites
SG Huang, K Vanmeensel, OJA Malek, O Van der Biest, J Vleugels
Materials science and engineering: A 528 (3), 1302-1309, 2011
1552011
Environmental assessment of solid state recycling routes for aluminium alloys: can solid state processes significantly reduce the environmental impact of aluminium recycling?
JR Duflou, AE Tekkaya, M Haase, T Welo, K Vanmeensel, K Kellens, ...
Cirp Annals 64 (1), 37-40, 2015
1402015
Binderless WC and WC–VC materials obtained by pulsed electric current sintering
SG Huang, K Vanmeensel, O Van der Biest, J Vleugels
International Journal of Refractory Metals and Hard Materials 26 (1), 41-47, 2008
1372008
Laser-based powder bed fusion additive manufacturing of pure copper
SD Jadhav, LR Goossens, Y Kinds, B Van Hooreweder, K Vanmeensel
Additive Manufacturing 42, 101990, 2021
1312021
Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg
P Van Cauwenbergh, V Samaee, L Thijs, J Nejezchlebová, P Sedlák, ...
Scientific reports 11 (1), 6423, 2021
1282021
3Y-TZP ceramics with improved hydrothermal degradation resistance and fracture toughness
F Zhang, K Vanmeensel, M Inokoshi, M Batuk, J Hadermann, ...
Journal of the European Ceramic Society 34 (10), 2453-2463, 2014
1242014
Critical influence of alumina content on the low temperature degradation of 2–3 mol% yttria-stabilized TZP for dental restorations
F Zhang, K Vanmeensel, M Inokoshi, M Batuk, J Hadermann, ...
Journal of the European Ceramic Society 35 (2), 741-750, 2015
1212015
VC, Cr3C2 and NbC doped WC–Co cemented carbides prepared by pulsed electric current sintering
SG Huang, L Li, K Vanmeensel, O Van der Biest, J Vleugels
International Journal of Refractory Metals and Hard Materials 25 (5-6), 417-422, 2007
1212007
Effect of temperature on the microstructure and tensile properties of micro-crack free hastelloy X produced by selective laser melting
ML Montero-Sistiaga, Z Liu, L Bautmans, S Nardone, G Ji, JP Kruth, ...
Additive Manufacturing 31, 100995, 2020
1132020
Hard, tough and strong ZrO2–WC composites from nanosized powders
G Anné, S Put, K Vanmeensel, D Jiang, J Vleugels, O Van der Biest
Journal of the European Ceramic Society 25 (1), 55-63, 2005
1102005
系统目前无法执行此操作,请稍后再试。
文章 1–20