Semiconducting and passive film properties of nitrogen-containing type 316LN stainless steels S Ningshen, UK Mudali, VK Mittal, HS Khatak Corrosion science 49 (2), 481-496, 2007 | 394 | 2007 |
On the pitting corrosion resistance of nitrogen alloyed cold worked austenitic stainless steels UK Mudali, P Shankar, S Ningshen, RK Dayal, HS Khatak, B Raj Corrosion Science 44 (10), 2183-2198, 2002 | 239 | 2002 |
Hydrogen effects on the passive film formation and pitting susceptibility of nitrogen containing type 316L stainless steels S Ningshen, UK Mudali, G Amarendra, P Gopalan, RK Dayal, HS Khatak Corrosion Science 48 (5), 1106-1121, 2006 | 126 | 2006 |
Influence of Si and Sb additions on the corrosion behavior of AZ91 magnesium alloy A Srinivasan, S Ningshen, UK Mudali, UTS Pillai, BC Pai Intermetallics 15 (12), 1511-1517, 2007 | 123 | 2007 |
Corrosion assessment of nitric acid grade austenitic stainless steels S Ningshen, UK Mudali, G Amarendra, B Raj Corrosion Science 51 (2), 322-329, 2009 | 116 | 2009 |
Corrosion behaviour of AISI type 304L stainless steel in nitric acid media containing oxidizing species S Ningshen, UK Mudali, S Ramya, B Raj Corrosion Science 53 (1), 64-70, 2011 | 114 | 2011 |
Corrosion behavior and surface film characterization of TaNbHfZrTi high entropy alloy in aggressive nitric acid medium J Jayaraj, C Thinaharan, S Ningshen, C Mallika, UK Mudali Intermetallics 89, 123-132, 2017 | 104 | 2017 |
Weld overlay coating of Inconel 617 M on type 316 L stainless steel by cold metal transfer process P Varghese, E Vetrivendan, MK Dash, S Ningshen, M Kamaraj, ... Surface and Coatings Technology 357, 1004-1013, 2019 | 87 | 2019 |
Hydrogen effects on pitting corrosion and semiconducting properties of nitrogen-containing type 316L stainless steel S Ningshen, UK Mudali Electrochimica acta 54 (26), 6374-6382, 2009 | 68 | 2009 |
Effect of anodization parameters on the structural morphology of titanium in fluoride containing electrolytes K Indira, S Ningshen, UK Mudali, N Rajendran Materials characterization 71, 58-65, 2012 | 65 | 2012 |
Corrosion performance and surface analysis of Ti–Ni–Pd–Ru–Cr alloy in nitric acid solution S Ningshen, M Sakairi, K Suzuki, T Okuno Corrosion Science 91, 120-128, 2015 | 60 | 2015 |
The corrosion resistance and passive film compositions of 12% Cr and 15% Cr oxide dispersion strengthened steels in nitric acid media S Ningshen, M Sakairi, K Suzuki, S Ukai Corrosion Science 78, 322-334, 2014 | 60 | 2014 |
Corrosion behaviour of nitrogen ion implanted AISI type 304L stainless steel in nitric acid medium N Padhy, S Ningshen, BK Panigrahi, UK Mudali Corrosion science 52 (1), 104-112, 2010 | 50 | 2010 |
Influence of oxygen ion irradiation on the corrosion aspects of Ti-5% Ta-2% Nb alloy and oxide coated titanium S Ningshen, UK Mudali, P Mukherjee, A Sarkar, P Barat, N Padhy, B Raj Corrosion science 50 (8), 2124-2134, 2008 | 45 | 2008 |
Corrosion behavior of Zr-based metallic glass coating on type 304L stainless steel by pulsed laser deposition method S Ningshen, UK Mudali, R Krishnan, B Raj Surface and Coatings Technology 205 (15), 3961-3966, 2011 | 44 | 2011 |
Diffusion behaviour of hydrogen in nitrogen containing austenitic alloys S Ningshen, M Uhlemann, F Schneider, HS Khatak Corrosion science 43 (12), 2255-2264, 2001 | 42 | 2001 |
Influence of metallurgical and chemical variables on the pitting corrosion behaviour of nitrogen-bearing austenitic stainless steels U Kamachi Mudali, S Ningshen, AK Tyagi, RK Dayal Materials science forum 318, 495-502, 1999 | 38 | 1999 |
The passive film characterization and anodic polarization behavior of 11% Cr ferritic/martensitic and 15% Cr oxide dispersion strengthened steels in different electrolytic … S Ningshen, M Sakairi, K Suzuki, S Ukai Applied surface science 274, 345-355, 2013 | 37 | 2013 |
Materials development and corrosion issues in the back end of fuel cycle UK Mudali, A Ravishankar, S Ningshen, G Suresh, R Sole, K Thyagarajan Energy Procedia 7, 468-473, 2011 | 35 | 2011 |
Microstructural analysis and corrosion behaviour of D9 stainless steel–Zirconium metal waste form alloys LR Bairi, S Ningshen, UK Mudali, B Raj Corrosion science 52 (7), 2291-2302, 2010 | 35 | 2010 |