The role of crystalline, mobile amorphous and rigid amorphous fractions in the performance of recycled poly (ethylene terephthalate)(PET) JD Badia, E Strömberg, S Karlsson, A Ribes-Greus Polymer degradation and stability 97 (1), 98-107, 2011 | 214 | 2011 |
Mechanical recycling of polylactide, upgrading trends and combination of valorization techniques JD Badia, A Ribes-Greus European Polymer Journal 84, 22-39, 2016 | 137 | 2016 |
Material valorisation of amorphous polylactide. Influence of thermo-mechanical degradation on the morphology, segmental dynamics, thermal and mechanical performance JD Badia, E Strömberg, S Karlsson, A Ribes-Greus Polymer degradation and stability 97 (4), 670-678, 2012 | 135 | 2012 |
Thermal analysis as a quality tool for assessing the influence of thermo-mechanical degradation on recycled poly (ethylene terephthalate) JD Badia, F Vilaplana, S Karlsson, A Ribes-Greus Polymer Testing 28 (2), 169-175, 2009 | 135 | 2009 |
Long-term properties and end-of-life of polymers from renewable resources JD Badia, O Gil-Castell, A Ribes-Greus Polymer Degradation and Stability 137, 35-57, 2017 | 130 | 2017 |
Hydrothermal ageing of polylactide/sisal biocomposites. Studies of water absorption behaviour and Physico-Chemical performance O Gil-Castell, JD Badia, T Kittikorn, E Strömberg, A Martínez-Felipe, M Ek, ... Polymer degradation and stability 108, 212-222, 2014 | 94 | 2014 |
Hygrothermal ageing of reprocessed polylactide JD Badia, L Santonja-Blasco, A Martínez-Felipe, A Ribes-Greus Polymer degradation and stability 97 (10), 1881-1890, 2012 | 79 | 2012 |
Impact of hydrothermal ageing on the thermal stability, morphology and viscoelastic performance of PLA/sisal biocomposites O Gil-Castell, JD Badia, T Kittikorn, E Strömberg, M Ek, S Karlsson, ... Polymer degradation and stability 132, 87-96, 2016 | 77 | 2016 |
Assessing the MALDI-TOF MS sample preparation procedure to analyze the influence of thermo-oxidative ageing and thermo-mechanical degradation on poly (lactide) JD Badia, E Strömberg, A Ribes-Greus, S Karlsson European Polymer Journal 47 (7), 1416-1428, 2011 | 76 | 2011 |
Thermal analysis applied to the characterization of degradation in soil of polylactide: II. On the thermal stability and thermal decomposition kinetics JD Badia, L Santonja-Blasco, R Moriana, A Ribes-Greus Polymer Degradation and Stability 95 (11), 2192-2199, 2010 | 72 | 2010 |
Water absorption and hydrothermal performance of PHBV/sisal biocomposites JD Badia, T Kittikorn, E Strömberg, L Santonja-Blasco, A Martínez-Felipe, ... Polymer degradation and stability 108, 166-174, 2014 | 65 | 2014 |
A statistical design of experiments for optimizing the MALDI-TOF-MS sample preparation of polymers. An application in the assessment of the thermo-mechanical degradation … JD Badia, E Strömberg, A Ribes-Greus, S Karlsson Analytica chimica acta 692 (1-2), 85-95, 2011 | 61 | 2011 |
Thermal analysis applied to the characterization of degradation in soil of polylactide: I. Calorimetric and viscoelastic analyses L Santonja-Blasco, R Moriana, JD Badía, A Ribes-Greus Polymer Degradation and Stability 95 (11), 2185-2191, 2010 | 61 | 2010 |
Thermal and thermo-oxidative stability of reprocessed poly (ethylene terephthalate) JD Badia, A Martinez-Felipe, L Santonja-Blasco, A Ribes-Greus Journal of analytical and applied pyrolysis 99, 191-202, 2013 | 60 | 2013 |
Relevant factors for the eco-design of polylactide/sisal biocomposites to control biodegradation in soil in an end-of-life scenario JD Badia, E Strömberg, T Kittikorn, M Ek, S Karlsson, A Ribes-Greus Polymer Degradation and Stability 143, 9-19, 2017 | 56 | 2017 |
Workshops of Innovation in Chemical Engineering to train communication skills in science and technology P San-Valero, A Robles, MV Ruano, N Martí, A Cháfer, JD Badia Education for Chemical Engineers, 2018 | 55 | 2018 |
Polylactide-based self-reinforced composites biodegradation: Individual and combined influence of temperature, water and compost O Gil-Castell, JD Badia, S Ingles-Mascaros, R Teruel-Juanes, A Serra, ... Polymer Degradation and Stability 158, 40-51, 2018 | 51 | 2018 |
A methodology to assess the energetic valorization of bio-based polymers from the packaging industry: Pyrolysis of reprocessed polylactide JD Badia, L Santonja-Blasco, A Martinez-Felipe, A Ribes-Greus Bioresource technology 111, 468-475, 2012 | 43 | 2012 |
Effect of sisal and hydrothermal ageing on the dielectric behaviour of polylactide/sisal biocomposites JD Badia, P Reig-Rodrigo, R Teruel-Juanes, T Kittikorn, E Strömberg, ... Composites Science and Technology 149, 1-10, 2017 | 41 | 2017 |
Electrospun Poly (ethylene-co-vinyl alcohol)/Graphene Nanoplatelets Composites of Interest in Intelligent Food Packaging Applications S Torres-Giner, Y Echegoyen, R Teruel-Juanes, J Badia, A Ribes-Greus, ... Nanomaterials 8 (10), 745, 2018 | 37 | 2018 |