Superplastic flow of fine‐grained yttria‐stabilized zirconia polycrystals: Constitutive equation and deformation mechanisms M Jiménez‐Melendo, A Domínguez‐Rodríguez, A Bravo‐León Journal of the American Ceramic Society 81 (11), 2761-2776, 1998 | 304 | 1998 |
Towards physical properties tailoring of carbon nanotubes-reinforced ceramic matrix composites ADR E. Zapata-Solvas , D. Gómez-García Journal of the european ceramic society 32, 3001-3020, 2012 | 237 | 2012 |
Characterisation and high temperature mechanical properties of zirconium boride-based materials GP J.J. Mele´ndez-Martı´neza,, A. Domı´nguez-Rodrı´gueza, F. Monteverdeb, C ... Journal of the European Ceramic Society 22, 2543–2549, 2002 | 209 | 2002 |
Effect of spark plasma sintering parameters on microstructure and room-temperature hardness and toughness of fine-grained boron carbide (B4C) BM Moshtaghioun, FL Cumbrera-Hernández, D Gómez-García, ... Journal of the european ceramic society 33 (2), 361-369, 2013 | 143 | 2013 |
Grain size dependence of hardness and fracture toughness in pure near fully-dense boron carbide ceramics BM Moshtaghioun, D Gomez-Garcia, A Dominguez-Rodriguez, RI Todd Journal of the European Ceramic Society 36 (7), 1829-1834, 2016 | 141 | 2016 |
Toughening of super-hard ultra-fine grained B4C densified by spark-plasma sintering via SiC addition BM Moshtaghioun, AL Ortiz, D Gómez-García, A Domínguez-Rodríguez Journal of the european ceramic society 33 (8), 1395-1401, 2013 | 138 | 2013 |
Microstructure–mechanical properties correlation in siliconized silicon carbide ceramics JM Fernández, A Munoz, AR de Arellano López, FMV Feria, ... Acta Materialia 51 (11), 3259-3275, 2003 | 137 | 2003 |
Plastic Deformation and Solid‐Solution Hardening of Y2O3‐Stabilized ZrO2 A Dominguez‐Rodriguez, KPD Lagerlöf, AH Heuer Journal of the American Ceramic Society 69 (3), 281-284, 1986 | 121 | 1986 |
Indentation Studies on Y2O2‐Stabilized ZrO2: I, Development of Indentation‐Induced Cracks MS Kaliszewski, G Behrens, AH Heuer, MC Shaw, DB Marshall, ... Journal of the American Ceramic Society 77 (5), 1185-1193, 1994 | 117 | 1994 |
Ionic conductivity of –12 mol % single crystals JD Solier, I Cachadina, A Dominguez-Rodriguez Physical Review B 48 (6), 3704, 1993 | 111 | 1993 |
Creep of silicon nitride ADR J.J. Melendez-Martınez Progress in Materials Science 49, 19-107, 2004 | 108 | 2004 |
Rapid carbothermic synthesis of silicon carbide nano powders by using microwave heating BM Moshtaghioun, R Poyato, FL Cumbrera, S de Bernardi-Martin, ... Journal of the european ceramic society 32 (8), 1787-1794, 2012 | 98 | 2012 |
Ultra-fast and energy-efficient sintering of ceramics by electric current concentration RI Zapata, E., Gomez, D., Dominguez-rodriguez, A., Todd Scientific Reports 5 (8513; DOI:10.1038/srep08513), 2015 | 88 | 2015 |
High‐temperature creep of yttria‐stabilized zirconia single crystals J Martinez‐Fernandez, M Jimenez‐Melendo, A Dominguez‐Rodriguez, ... Journal of the American Ceramic Society 73 (8), 2452-2456, 1990 | 86 | 1990 |
High temperature mechanical characteristics of superplastic yttria-stabilized zirconia. An examination of the flow process A Jiménez-Melendo, M.,Domínguez-Rodríguez Acta Materialia 48 (12), 3201-3210, 2000 | 81* | 2000 |
Indentation Studies on Y2O3‐Stabilized ZrO2: II, Toughness Determination from Stable Growth of Indentation‐Induced Cracks GW Dransmann, RW Steinbrech, A Pajares, F Guiberteau, ... Journal of the American Ceramic Society 77 (5), 1194-1201, 1994 | 80 | 1994 |
Densification of additive-free polycrystalline β-SiC by spark-plasma sintering A Lara, AL Ortiz, A Muñoz, A Domínguez-Rodríguez Ceramics International 38 (1), 45-53, 2012 | 73 | 2012 |
Low‐Temperature Ionic Conductivity of 9.4‐mol%‐Yttria‐Stabilized Zirconia Single Crystals J de Dios Solier, MA Pérez‐Jubindo, A Dominguez‐Rodriguez, AH Heuer Journal of the American Ceramic Society 72 (8), 1500-1502, 1989 | 67 | 1989 |
Densification of B4C nanopowder with nanograin retention by spark-plasma sintering BM Moshtaghioun, AL Ortiz, D Gomez-Garcia, A Dominguez-Rodriguez Journal of the European Ceramic Society 35 (6), 1991-1998, 2015 | 66 | 2015 |
High-temperature precipitation hardening of Y2O3 partially-stabilized ZrO2 (Y-PSZ) single crystals AH Heuer, V Lanteri, A Dominguez-Rodriguez Acta metallurgica 37 (2), 559-567, 1989 | 65 | 1989 |