The preparation of SiC ultrafine fibers containing low amount of oxygen by the electrospinning and pyrolysis of vinyl-modified polycarbosilane

B Yao, B Lu, Q Huang, ZR Huang, Q Yuan - Ceramics International, 2020 - Elsevier
The high-temperature stability of the SiC ultrafine fibers is limited by the massive amounts of
oxygen introduced during the oxidative curing process. In this study, vinyl-modified …

Large-scale preparation of SiBN ceramic fibres from a single source precursor

YQ Peng, KQ Han, X Zhao, MH Yu - Ceramics International, 2014 - Elsevier
Large-scale production of SiBN ceramic fibres was achieved by the pyrolysis of N-
methylpolyborosilazane. This precursor was prepared by a three-step synthesis starting from …

Oxygen-free ceramic fibers from organosilicon precursors and E-beam curing

H Ichikawa, K Okamura, T Sequchi - 1995 - osti.gov
Oxygen free Si-C fibers {open_quotes} Hi-Nicalon {close_quotes} with C/Si ratio of 1.39 and
{open_quotes} Hi-Nicalon S {close_quotes} with C/Si ratio of 1.05 were synthesized from …

Polymer derived SiBCN (O) ceramics with tunable element content

B Wang, Y Song, X Zhang, K Chen, M Liu, X Hu… - Ceramics …, 2022 - Elsevier
SiBCN ceramics have excellent high-temperature stability and anti-oxidation properties, and
they are candidates for materials used at extreme conditions. In this paper, amorphous …

Preparation of C/SiBCN composites by precursor infiltration and pyrolysis using a novel precursor

Y Jia, X Ji, Y Gou, Y Li, H Hu - Materials Research Express, 2019 - iopscience.iop.org
A novel polyborosilazane (PBSZ) precursor was synthesized via single source precursor
route, in which B existed in the form of B–N hexatomic ring in the main chain. The …

Polymer derived ZrO2 reinforced SiC-ZrB2 polycrystalline fiber

P Zhang, Z Zheng, K Zhuang, C Sun, Z Yu… - Journal of the European …, 2022 - Elsevier
Most polycrystalline SiC-based fibers were prepared at a sintering temperature higher than
1600° C. In this work, a ZrO 2 reinforced SiC-ZrB 2 polycrystalline fiber was prepared at …

Preparation of C–SiC/ZrSixOyCz core-shell fibers by Coaxial electrospinning and the high-temperature performance

J Rui, J Li, Y Li, H Liu, Y Zhang, J Huang, P Ma… - Ceramics …, 2022 - Elsevier
Core-shell ceramics fibers with multiple composition are ideal candidates for thermal
insulation application at high temperature. Herein, ultrathin C–SiC/ZrSi x O y C z core-shell …

Synthesis of β‐SiC Fine Fibers by the Forcespinning Method with Microwave Irradiation

A Salinas, M Lizcano, K Lozano - Journal of Ceramics, 2015 - Wiley Online Library
A rapid method for synthesizing β‐silicon carbide (β‐SiC) fine fiber composite has been
achieved by combining forcespinning technology with microwave energy processing. β‐SiC …

Modification of polycarbosilane by polyborazine as a precursor for oxygen-free SiC fibers

F Cao, X Li, J Ryu, D Kim - Journal of Materials Chemistry, 2003 - pubs.rsc.org
Infusible but soluble polycarbosilane (PCS) was obtained by heating Yajima PCS at 300° C
for 1 h with 1–wt.% of polyborazine (PBN). The simple addition of PBN to PCS and …

Effect of Hf and B incorporation on the SiOC precursor architecture and high-temperature oxidation behavior of SiHfBOC ceramics

Y Lyu, H Tang, G Zhao - Journal of the European Ceramic Society, 2020 - Elsevier
Abstract Polymer-derived ceramics (PDCs), such as silicon oxycarbide and its derivatives,
show an exceptional high oxidative stability under extreme conditions. A novel …