Gaseous Corrosion of Metals in a 60% H2 O, 40% HCl Environment
JP Carter, BS Covino Jr, TJ Driscoll, WD Riley… - …, 1984 - meridian.allenpress.com
Laboratory tests were conducted on iron, nickel, titanium, and cobalt base alloys and
zirconium 702, primarily at temperatures of 95 to 400 C for exposure periods of 15 days in a …
zirconium 702, primarily at temperatures of 95 to 400 C for exposure periods of 15 days in a …
[引用][C] Gaseous corrosion of metals in a 60% H2O, 40% HCl environment
JP CARTER, BS COVINO Jr… - Corrosion …, 1984 - pascal-francis.inist.fr
Gaseous corrosion of metals in a 60% H2O, 40% HCl environment CNRS Inist Pascal-Francis
CNRS Pascal and Francis Bibliographic Databases Simple search Advanced search Search …