Determination of elastic modulus of thin layers using nanoindentation

J Menčík, D Munz, E Quandt, ER Weppelmann… - Journal of Materials …, 1997 - Springer
Elastic modulus of thin homogeneous films can be determined by indenting the specimen to
various depths and extrapolating the measured (apparent) E-values to zero penetration. The
paper shows the application of five approximation functions for this purpose: linear,
exponential, reciprocal exponential, Gao's, and the Doerner and Nix functions. Comparison
of the results for 26 film/substrate combinations has shown that the indentation response of
film/substrate composites can, in general, be described by the Gao analytical function. In …

Determination of elastic modulus of thin layers

J Menčik, D Munz, E Quandt, A Ludwig - International Journal of …, 1999 - degruyter.com
Der Elastizitätsmodul dünner metallischer oder keramischer Schichten (Dicke 0.1 bis 10|
nm) kann mit verschiedenen Methoden bestimmt werden. In diesem Aufsatz werden drei
Methoden diskutiert: Nanoindentation, Balkenbiegung und Balkenresonanzmethode. Das
Prinzip jeder Methode wird erklärt und die Vorteile und Nachteile zusammengefaßt. Auch
werden praktische Hinweise gegeben, die aufgrund von Messungen an
hochmagnetostriktiven TbFe/FeCo-Viellagenschichten gewonnen wurden.