Influence of ECAP process on mechanical and corrosion properties of pure Mg and ZK60 magnesium alloy for biodegradable stent applications

E Mostaed, M Vedani, M Hashempour, M Bestetti - Biomatter, 2014 - Taylor & Francis
Equal channel angular pressing (ECAP) was performed on ZK60 alloy and pure Mg in the
temperature range 150–250° C. A significant grain refinement was detected after ECAP …

High strength and fatigue properties of Mg-Zn-Ca alloys after severe plastic deformation

E Vasilev, VI Kopylov, ML Linderov, AI Brilevsky… - 2019 - ntnuopen.ntnu.no
Magnesium alloys are the lightest metallic structural materials with an outstanding specific
strength. This makes them appealing for a wide range of applications in “green” …

Effect of Microstructure Refinement on the Corrosion Behavior of the Bioresorbable Mg-1Zn-0.2 Ca and Mg-1Ca Alloys

OB Kulyasova, GD Khudododova, GS Dyakonov… - Materials, 2022 - mdpi.com
This paper presents a comprehensive study of the effect of the processing by high-pressure
torsion (HPT) on the corrosion behavior in Ringer's solution for two popular bioresorbable …

[HTML][HTML] The effect of severe plastic deformation on the Mg properties after CEC deformation

B Sułkowski, M Janoska, G Boczkal, R Chulist… - Journal of Magnesium …, 2020 - Elsevier
In this study, the effect of severe plastic deformation on the Mg grain refinement and
recovery mechanism was investigated. Technical pure magnesium was deformed at room …

Effect of equal channel angular pressing on microstructure, texture, and high-cycle fatigue performance of wrought magnesium alloys

J Müller, M Janeček, S Yi, J Čížek… - International journal of …, 2009 - degruyter.com
The magnesium alloys AZ80 und ZK60 received from Dead Sea Magnesium in as-cast
conditions were extruded at T= 350° C using an extrusion ratio of ER= 22. The extruded bars …

Effect of high-pressure torsion on grain refinement, strength enhancement and uniform ductility of EZ magnesium alloy

K Bryła, J Morgiel, M Faryna, K Edalati, Z Horita - Materials Letters, 2018 - Elsevier
Strength enhancement of Mg-based alloys without deteriorating their ductility is currently a
major scientific and industrial challenge. In this study, discs of as-cast EZ33A alloy were …

Microstructures and mechanical properties of Mg alloy after severe torsion straining process

Y Miyahara, N Emi, K Neishi, K Nakamura… - Materials Science …, 2006 - Trans Tech Publ
Grain refinement is attempted using severe plastic deformation (SPD) through the severe
torsion straining process (STSP) which we have developed recently. The STSP is a …

Enhancement of the Mechanical Properties of an Mg–Zn–Ca Alloy Using High‐Pressure Torsion

OB Kulyasova, RK Islamgaliev, Y Zhao… - Advanced …, 2015 - Wiley Online Library
The structure and properties of an Mg–Zn–Ca alloy processed by high‐pressure torsion
(HPT) are investigated. Microstructure is studied by transmission electron microscopy …

Effect of temperature on the processing of a magnesium alloy by high-pressure torsion

Y Huang, RB Figueiredo, T Baudin, AL Helbert… - Journal of Materials …, 2012 - Springer
It is now well known that processing by SPD can significantly increase the strength of
metallic materials by refining the grain structure and increasing the density of defects. The …

[HTML][HTML] The effect of Equal Channel Angular Pressing on the stress corrosion cracking susceptibility of AZ31 alloy in simulated body fluid

M Peron, PC Skaret, A Fabrizi, A Varone… - journal of the …, 2020 - Elsevier
Despite the great potential of Mg and its alloys as material for biodegradable implants, their
low resistance to the simultaneous action of corrosion and mechanical stresses in the …