Analysis of mechanical stress due to winding pretension in a 1.5 T superconducting MRI magnet
The paper presents the analysis of stresses due to winding tension in a 1.5 T MRI magnet
with a clear bore of∼ 1 m and an outer diameter of∼ 1.8 m. The magnet has four pairs of …
with a clear bore of∼ 1 m and an outer diameter of∼ 1.8 m. The magnet has four pairs of …
Analysis of mechanical stress due to winding pretension in a 1.5 T superconducting MRI magnet
SR Thekkethil, S Kar, N Suman, M Kumar, V Soni… - 2018 - indianjournals.com
The paper presents the analysis of stresses due to winding tension in a 1.5 T MRI magnet
with a clear bore of∼ 1 m and an outer diameter of∼ 1.8 m. The magnet has four pairs of …
with a clear bore of∼ 1 m and an outer diameter of∼ 1.8 m. The magnet has four pairs of …
Analysis of mechanical stress due to winding pretension in a 1.5 T superconducting MRI magnet
SR Thekkethil, S Kar, N Suman, M Kumar, V Soni… - 2018 - indianjournals.com
The paper presents the analysis of stresses due to winding tension in a 1.5 T MRI magnet
with a clear bore of∼ 1 m and an outer diameter of∼ 1.8 m. The magnet has four pairs of …
with a clear bore of∼ 1 m and an outer diameter of∼ 1.8 m. The magnet has four pairs of …