Cemented carbide phase diagrams: A review
CM Fernandes, AMR Senos - … Journal of Refractory Metals and Hard …, 2011 - Elsevier
One of the main topics of the actual research in the field of cemented carbides concerns the
development of new composites, with partial or total substitution of the traditional cobalt …
development of new composites, with partial or total substitution of the traditional cobalt …
Defect chemistry and electrical characteristics of undoped and Mn-doped ZnO
J Han, PQ Mantas, AMR Senos - Journal of the European Ceramic Society, 2002 - Elsevier
Undoped and Mn-doped ZnO samples were sintered at 1373, 1473, and 1573 K, for 2 h, in
air, and then quenched to room temperature. Defect concentrations in these samples at the …
air, and then quenched to room temperature. Defect concentrations in these samples at the …
Digital tools for material selection in product design
PS Ramalhete, AMR Senos, C Aguiar - Materials & Design (1980-2015), 2010 - Elsevier
The increasing number of normalized materials, promoters and users led to a significant
amount and diversity of databases and software for material selection, presenting differentiating …
amount and diversity of databases and software for material selection, presenting differentiating …
Effect of Al and Mn doping on the electrical conductivity of ZnO
J Han, PQ Mantas, AMR Senos - Journal of the European Ceramic Society, 2001 - Elsevier
Samples of Al-doped and Mn-doped ZnO with a doping level up to 1.2 mol% were sintered
at temperatures from 1100 to 1400C in air. dc Electrical conductivities of these samples at …
at temperatures from 1100 to 1400C in air. dc Electrical conductivities of these samples at …
Phase coexistence region and dielectric properties of PZT ceramics
MR Soares, AMR Senos, PQ Mantas - Journal of the European Ceramic …, 2000 - Elsevier
In PZT ceramics it is commonly observed that the tetragonal and the rhombohedral phases
may coexist around the morphotropic phase boundary (MPB). Some controversy still exists …
may coexist around the morphotropic phase boundary (MPB). Some controversy still exists …
Corrosion behaviour of WC hardmetals with nickel-based binders
…, CM Fernandes, E Soares, J Sacramento, AMR Senos… - Corrosion …, 2019 - Elsevier
Cobalt is the standard binder in tungsten carbide (WC) hardmetals due to its compatibility
with the WC phase, resulting in composites with exceptional hardness and wear resistance. …
with the WC phase, resulting in composites with exceptional hardness and wear resistance. …
Grain growth in Mn-doped ZnO
J Han, PQ Mantas, AMR Senos - Journal of the European Ceramic Society, 2000 - Elsevier
Grain growth in ZnO doped with 0.1 to 1.2 mol% Mn was investigated during isothermal sintering
from 1100 to 1300C in air. Mn doping promotes the grain growth of ZnO during sintering…
from 1100 to 1300C in air. Mn doping promotes the grain growth of ZnO during sintering…
Varistor behaviour of Mn-doped ZnO ceramics
J Han, AMR Senos, PQ Mantas - Journal of the European Ceramic Society, 2002 - Elsevier
Polycrystalline ZnO doped with MnO, from 0.1 to 0.6 mol%, was prepared by conventional
ceramic processing. The effect of Mn doping on the electrical properties of ZnO was …
ceramic processing. The effect of Mn doping on the electrical properties of ZnO was …
Wet synthesis and characterization of modified hydroxyapatite powders
Hydroxyapatite powders with reproducibly different Ca/P ratios and powders with varying
amounts of co-precipitated magnesium, sodium and potassium were synthesized by a wet …
amounts of co-precipitated magnesium, sodium and potassium were synthesized by a wet …
Densification and grain growth of Al-doped ZnO
J Han, PQ Mantas, AMR Senos - Journal of Materials Research, 2001 - cambridge.org
The densification and grain growth of ZnO doped with Al from 0.08 to 1.2 mol% were
investigated during isothermal sintering between 1100 and 1400 C. The Al dopant significantly …
investigated during isothermal sintering between 1100 and 1400 C. The Al dopant significantly …