Dislocation dynamics in a nickel-based superalloy via in-situ transmission scanning electron microscopy

JC Stinville, ER Yao, PG Callahan, J Shin, F Wang… - Acta Materialia, 2019 - Elsevier
Acta Materialia, 2019Elsevier
Micro-tensile specimens of nickel-based superalloy oligocrystals were tested in-situ in an
scanning electron microscope in transmission mode (TSEM) enabling observation of
dislocations. The dynamics of dislocation motion during tensile loading were captured and
correlated with the measured intermittencies during plastic flow recorded by high load-and
temporal-resolution sensors. This investigation in particular focused on the dislocation
behavior near twin boundaries with different slip configurations. A multiplicity of deformation …
Abstract
Micro-tensile specimens of nickel-based superalloy oligocrystals were tested in-situ in an scanning electron microscope in transmission mode (TSEM) enabling observation of dislocations. The dynamics of dislocation motion during tensile loading were captured and correlated with the measured intermittencies during plastic flow recorded by high load- and temporal-resolution sensors. This investigation in particular focused on the dislocation behavior near twin boundaries with different slip configurations. A multiplicity of deformation mechanisms at the dislocation scale were observed within individual slip bands, including precipitate shearing, dislocation decorrelation and antiphase boundary-coupled shearing. These processes affect strain localization near twin boundaries and provide new defect-level insights on plastic localization and fatigue crack initiation in these alloys.
Elsevier