Fabrication of Bi0.5(Na0.4K0.1)TiO3 Lead-Free Ceramics Using Reactive Templated Grain Growth Method for Improving Their Preferred Degree of Orientation …

LD Vuong, DA Quang, P Van Quan… - Journal of Electronic …, 2020 - Springer
Abstract A Bi 4 Ti 3 O 12 template was added to the (1− x)[Bi 0.5 (Na 0.4 K 0.1) TiO 3]-x Bi 4
Ti 3 O 12 ceramics (BNKT; where x= 0, 0.1, 0.15, 0.20, 0.25, and 0.30) and lead-free …

Fabrication of Bi0. 5 (Na0. 4K0. 1) TiO3 Lead-Free Ceramics Using Reactive Templated Grain Growth Method for Improving Their Preferred Degree of Orientation …

LD Vuong, DA Quang, P Van Quan… - Journal of Electronic …, 2020 - search.ebscohost.com
Abstract A Bi< sub> 4</sub> Ti< sub> 3</sub> O< sub> 12</sub> template was added to the
(1− x)[Bi< sub> 0.5</sub>(Na< sub> 0.4</sub> K< sub> 0.1</sub>) TiO< sub> 3</sub>]-xBi< …

[PDF][PDF] Fabrication of Bi0. 5 (Na0. 4K0.) TiO3 Lead-Free Ceramics Using Reactive Templated Grain Growth Method for Improving Their Preferred Degree of Orientation …

N TRUONG-THO - csdlkhoahoc.hueuni.edu.vn
A Bi4Ti3O12 template was added to the (1 À x)[Bi0. 5 (Na0. 4K0. 1) TiO3]-xBi4-Ti3O12
ceramics (BNKT; where x= 0, 0.1, 0.15, 0.20, 0.25, and 0.30) and leadfree ceramics were …

Fabrication of Bi0.5(Na0.4K0.1)TiO3 Lead-Free Ceramics Using Reactive Templated Grain Growth Method for Improving Their Preferred Degree of Orientation …

LD Vuong, DA Quang, P Van Quan… - Journal of Electronic …, 2020 - ui.adsabs.harvard.edu
Abstract A Bi 4 Ti 3 O 12 template was added to the (1-x)[Bi 0.5 (Na 0.4 K 0.1) TiO 3]-xBi 4 Ti
3 O 12 ceramics (BNKT; where x= 0, 0.1, 0.15, 0.20, 0.25, and 0.30) and lead-free ceramics …