Kinetics of high temperature oxidation and chromia volatilization for a binary Ni–Cr alloy
P Berthod - Oxidation of Metals, 2005 - Springer
The volatilization of the external chromia layer formed by oxidation of a Ni–30Cr alloy was
studied at 1000, 1100, 1200 and 1300° C. This was done by analyzing the mass gain curves …
studied at 1000, 1100, 1200 and 1300° C. This was done by analyzing the mass gain curves …
Corrosion of glass contact refractories for the vitrification of radioactive wastes: a review
A key consideration for all radioactive waste vitrification technologies is the physical and
chemical integrity of the melting vessel. Most melting vessels require refractory liners that …
chemical integrity of the melting vessel. Most melting vessels require refractory liners that …
[HTML][HTML] Electrolysis of iron in a molten oxide electrolyte
J Wiencke, H Lavelaine, PJ Panteix, C Petitjean… - Journal of Applied …, 2018 - Springer
Direct iron production at molten metal state from iron oxides by the sole application of
electrical energy represents a possible route to decarbonize steel industry. Although …
electrical energy represents a possible route to decarbonize steel industry. Although …
Electrolysis of molten iron oxide with an iridium anode: the role of electrolyte basicity
H Kim, J Paramore, A Allanore… - Journal of The …, 2011 - iopscience.iop.org
Molten oxide electrolysis (MOE) is a carbon-free, electrochemical technique to decompose a
metal oxide directly into liquid metal and oxygen gas. From an environmental perspective …
metal oxide directly into liquid metal and oxygen gas. From an environmental perspective …
Molten salt induced corrosion of Inconel 625 superalloy in PbSO4–Pb3O4–PbCl2–Fe2O3–ZnO environment
EM Zahrani, AM Alfantazi - Corrosion Science, 2012 - Elsevier
Corrosion behavior of alloy 625 was studied in a molten salt consisting of 47PbSO4–23 ZnO–
13 Pb3O4–10Fe2O3–7PbCl2 (wt.%) under air atmosphere at 600, 700 and 800° C, utilizing …
13 Pb3O4–10Fe2O3–7PbCl2 (wt.%) under air atmosphere at 600, 700 and 800° C, utilizing …
Decomposition of persistent luminescent microparticles in corrosive phosphate glass melt
Findings on the decomposition of persistent luminescent (PeL) SrAl 2 O 4: Eu 2+, Dy 3+
microparticles (MPs) in phosphate glass melt under static condition are reported. PeL …
microparticles (MPs) in phosphate glass melt under static condition are reported. PeL …
Mechanical alloying of cold-sprayed Ni-Nb-Si composite coating by friction stir processing: Improvement in microstructure and resistance against molten silicates …
Y Xu, J Ge, B Ji, W Li - Surface and Coatings Technology, 2022 - Elsevier
In this study, for the first time the Ni-Nb-Si composite coating system was prepared on the
In718 superalloy substrate by solid-state cold spraying and modified by solid-state friction …
In718 superalloy substrate by solid-state cold spraying and modified by solid-state friction …
Influence of the phosphate glass melt on the corrosion of functional particles occurring during the preparation of glass-ceramics
We report our findings on the impact of the glass composition on the corrosion of
microparticles occurring during the preparation of glass-ceramics using the direct doping …
microparticles occurring during the preparation of glass-ceramics using the direct doping …
[HTML][HTML] Oxidation and electrical properties of chromium–iron alloys in a corrosive molten electrolyte environment
M Esmaily, AN Mortazavi, N Birbilis, A Allanore - Scientific Reports, 2020 - nature.com
Chromium–iron (CrFe) binary alloys have recently been proposed to serve as the “inert”
anode for molten oxide electrolysis (MOE). Herein, the effects of anodic polarization on …
anode for molten oxide electrolysis (MOE). Herein, the effects of anodic polarization on …
Differential aeration corrosion of silver in sulfate melts at 900° C
D Diomande, S Mathieu, PJ Panteix, M Siblani… - Corrosion …, 2023 - Elsevier
The thermodynamic of the Ag/Ag 2 SO 4 electrode, serving as reference for carrying
electrochemical experiences of corrosion in sulfates at 900° C, was investigated because of …
electrochemical experiences of corrosion in sulfates at 900° C, was investigated because of …