Hydriding of titanium: Recent trends and perspectives in advanced characterization and multiscale modeling

Y Zhu, TW Heo, JN Rodriguez, PK Weber, R Shi… - Current Opinion in Solid …, 2022 - Elsevier
Titanium (Ti) and its alloys are attractive for a wide variety of structural and functional
applications owing to excellent specific strength, toughness and stiffness, and corrosion …

Effect of hydrogen charging on microstructural evolution and corrosion behavior of Ti-4Al-2V-1Mo-1Fe alloy

Y Qiao, D Xu, S Wang, Y Ma, J Chen, Y Wang… - Journal of Materials …, 2021 - Elsevier
The effect of hydrogen charging on microstructural evolution and corrosion behavior of a Ti-
4Al-2V-1Mo-1Fe alloy in a 3.5 wt.% NaCl solution was investigated. The results showed that …

Resolving hydrogen atoms at metal-metal hydride interfaces

S de Graaf, J Momand, C Mitterbauer, S Lazar… - Science …, 2020 - science.org
Hydrogen as a fuel can be stored safely with high volumetric density in metals. It can,
however, also be detrimental to metals, causing embrittlement. Understanding fundamental …

The corrosion behaviour of candidate container materials for the disposal of high-level waste and spent fuel–a summary of the state of the art and opportunities for …

C Padovani, F King, C Lilja, D Féron… - Corrosion …, 2017 - journals.sagepub.com
This paper presents a state-of-the-art analysis of the expected degradation processes of a
variety of candidate container materials for the disposal of high-level waste and/or spent …

Effect of pretreatments on the hydrogen evolution kinetics of pure titanium using impedance and SECM technologies

XR Li, QH Zhang, XZ Meng, LK Wu, FH Cao - Corrosion Science, 2021 - Elsevier
The behaviors and kinetics of hydrogen evolution reaction (HER) on pure titanium
spontaneously passivated in air (P-Ti), activated by electrochemical method (EA-Ti) and …

The formation of hydride and its influence on Ti–6Al–4V alloy fracture behavior

H Zhang, C Leygraf, L Wen, F Huang, H Chang… - International Journal of …, 2023 - Elsevier
The fracture mechanism of hydrogen charged Ti–6Al–4V has been investigated through a
multianalytical approach. The difference in hydrogen solubility between β phase (high …

The influence of surface nanoroughness, texture and chemistry of TiZr implant abutment on oral biofilm accumulation

R Xing, SP Lyngstadaas, JE Ellingsen… - Clinical Oral …, 2015 - Wiley Online Library
Objectives The aim of the study was to examine surface nanoroughness, texture and
chemistry of dental implant abutment and to investigate how these parameters influence oral …

Electrochemical hydrogen permeation in wrought and electron beam melted Ti-6Al-4V alloys

M Hayoun, N Eliaz, NU Navi, N Lulu-Bitton, P Shekhter… - Corrosion …, 2024 - Elsevier
Abstract Ti-6Al-4V is one of the most widely used titanium alloys. However, it is susceptible
to hydrogen embrittlement, eg due to hydride formation. Hydrogen permeability through Ti …

Temperature-dependence corrosion behavior of Ti6Al4V in the presence of HCl

F Yu, O Addison, A Davenport - Frontiers in Materials, 2022 - frontiersin.org
Ti alloys have been widely used in biomedical field due to good compatibility and corrosion
resistance. However, corrosion-related failures of implanted Ti devices and prostheses have …

In situ studies of hydrogen evolution kinetics on pure titanium surface: The effects of pre-reduction and dissolved oxygen

XR Li, XZ Meng, QH Zhang, HR Cai… - The Journal of …, 2022 - ACS Publications
The apparent cathodic current on the Ti surface in acidic solution is composed of three
reactions: the reductions of the oxide film, H+, and O2. However, classical electrochemical …