Powder‐based additive manufacturing: A critical review of materials, methods, opportunities, and challenges
R Shanthar, K Chen, C Abeykoon - Advanced Engineering …, 2023 - Wiley Online Library
As a 0D material, powder particles can be used to create almost any complicated
engineering component by utilizing the high‐performance manufacturing capabilities of …
engineering component by utilizing the high‐performance manufacturing capabilities of …
Design of novel quasi-trivalent dual-main-phase Ce magnets with high performance by manipulating the chemical state of Ce
Abstract The application of Nd-Fe-B magnet with substitution of Nd by cheap and abundant
Ce elements is seriously limited due to the intrinsically inferior magnetic properties of Ce-Fe …
Ce elements is seriously limited due to the intrinsically inferior magnetic properties of Ce-Fe …
[HTML][HTML] A large-volume 3D EBSD study on additively manufactured 316L stainless steel
Most microstructure characterization tools are based on the observation of two-dimensional
(2D) sections through a material. The results allow, for microstructures with homogeneous …
(2D) sections through a material. The results allow, for microstructures with homogeneous …
3D Printing Technologies for Fabrication of Magnetic Materials Based on Metal–Polymer Composites: A Review
Additive manufacturing is a very rapidly developing industrial field. It opens many
possibilities for the fast fabrication of complex-shaped products and devices, including …
possibilities for the fast fabrication of complex-shaped products and devices, including …
A Novel Magnetic Hardening Mechanism for Nd‐Fe‐B Permanent Magnets Based on Solid‐State Phase Transformation
Permanent magnets based on neodymium‐iron‐boron (Nd‐Fe‐B) alloys provide the highest
performance and energy density, finding usage in many high‐tech applications. Their …
performance and energy density, finding usage in many high‐tech applications. Their …
Achieving excellent soft-magnetic properties in CoFeAlMnCr high entropy alloy by in-situ additive manufacturing
Additive manufacturing enables intricate designs for electrical machines. However, soft-
magnetic alloys produced through this method often fall short in magnetic performance …
magnetic alloys produced through this method often fall short in magnetic performance …
Tailoring the magnetic properties and microstructure of Alnico 8 magnets by various Ti contents and processing conditions
SU Rehman, C Wei, R Zhang, H Liu, S Li, Z Minglong… - Intermetallics, 2022 - Elsevier
Shape anisotropy, developed as a result of spinodal decomposition (SD) is the basis for the
hysteresis behavior of Alnico magnets. The SD process is sensitive to processing conditions …
hysteresis behavior of Alnico magnets. The SD process is sensitive to processing conditions …
Laser directed energy deposition of Alnico-8H from blended elemental powders: Effect of nickel increase on magnetic properties
S Dussa, SS Joshi, M Radhakrishnan… - Journal of Magnetism …, 2024 - Elsevier
Abstract Alnico-8H (14 wt% Ni) and Alnico-8H (19 wt% Ni) were additively fabricated from a
blend of elemental powders with compositions (in wt.%) of 38Co-29Fe-14Ni-8Al-8Ti-3Cu …
blend of elemental powders with compositions (in wt.%) of 38Co-29Fe-14Ni-8Al-8Ti-3Cu …
Relationships between the grain orientation, spinodal structure, and magnetic properties of AlNiCo alloys
Y Liu, H Luan, J Zhao, Z Zhao, L Liu, Y Ding… - Journal of Alloys and …, 2025 - Elsevier
With renewed interest in AlNiCo alloys due to the rare-earth crisis, advanced
characterization techniques have been used to gain more structural information for further …
characterization techniques have been used to gain more structural information for further …
High-performance Alnico magnets prepared by powder bed fusion
ZY Zhang, MJ Zhou, JB Sun, B Li, S Wang… - Journal of Alloys and …, 2024 - Elsevier
Fine-grained and anisotropic Alnico magnets were prepared by powder bed fusion using a
laser beam. The as-built magnets were treated by solution treatment (ST) at 1250° C …
laser beam. The as-built magnets were treated by solution treatment (ST) at 1250° C …