[HTML][HTML] First-principles study of metallic impurities induced 355 nm UV laser absorption in fused silica
To date, it is controversial which metallic impurities play crucial role in the laser induced
degradation and damage of fused silica at 355 nm. In this work, a First-principles study for …
degradation and damage of fused silica at 355 nm. In this work, a First-principles study for …
[PDF][PDF] 熔石英元件紫外脉冲激光辐照损伤特性研究进展综述
杨李茗, 黄进, 刘红婕, 王凤蕊, 耿峰, 孙来喜… - Acta Optica …, 2022 - researching.cn
摘要熔石英光学元件在高能量密度的紫外脉冲激光辐照下往往极易出现后表面损伤,
这严重影响了紫外高功率脉冲激光装置的可靠性. 综合国内外相关研究进展 …
这严重影响了紫外高功率脉冲激光装置的可靠性. 综合国内外相关研究进展 …
Subsurface defects of fused silica optics and laser induced damage at 351 nm
L Hongjie, H Jin, W Fengrui, Z Xinda, Y Xin… - Optics express, 2013 - opg.optica.org
Many kinds of subsurface defects are always present together in the subsurface of fused
silica optics. It is imperfect that only one kind of defects is isolated to investigate its impact on …
silica optics. It is imperfect that only one kind of defects is isolated to investigate its impact on …
Layer by layer exposure of subsurface defects and laser-induced damage mechanism of fused silica
B Li, C Hou, C Tian, J Guo, X Xiang, X Jiang… - Applied Surface …, 2020 - Elsevier
Inert ion beams with large incident angle were used for layer by layer etching of chemical-
mechanical polished fused silica. The evolution of the impurities, subsurface defects, surface …
mechanical polished fused silica. The evolution of the impurities, subsurface defects, surface …
Subsurface damage measurement of ground fused silica parts by HF etching techniques
J Neauport, C Ambard, P Cormont, N Darbois… - Optics express, 2009 - opg.optica.org
Detection and measurement of subsurface damage of ground optical surfaces are of major
concern in the assessment of high damage thresholds fused silica optics for high power …
concern in the assessment of high damage thresholds fused silica optics for high power …
Imaging subsurface damage of grinded fused silica optics by confocal fluorescence microscopy
J Neauport, P Cormont, P Legros, C Ambard… - Optics …, 2009 - opg.optica.org
We report an experimental investigation of fluorescence confocal microscopy as a tool to
measure subsurface damage on grinded fused silica optics. Confocal fluorescence …
measure subsurface damage on grinded fused silica optics. Confocal fluorescence …
Material response during nanosecond laser induced breakdown inside of the exit surface of fused silica
SG Demos, RA Negres, RN Raman… - Laser & Photonics …, 2013 - Wiley Online Library
The material response following nanosecond, UV laser induced breakdown inside of the exit
surface of fused silica is investigated using multimodal time resolved microscopy. The study …
surface of fused silica is investigated using multimodal time resolved microscopy. The study …
Subsurface defects characterization and laser damage performance of fused silica optics during HF-etched process
H Liu, X Ye, X Zhou, J Huang, F Wang, X Zhou, W Wu… - Optical Materials, 2014 - Elsevier
Subsurface defects of fused silica optics would vary with HF-etched process. In this paper,
the subsurface defects characteristics of HF-etched fused silica optics and their effects on …
the subsurface defects characteristics of HF-etched fused silica optics and their effects on …
[PDF][PDF] Progress in detection and suppression techniques for processing-induced sub-surface defects of fused silica optical elements
陈明君, 王会尧, 程健, 赵林杰, 杨浩, 刘启… - Journal of mechanical …, 2021 - qikan.cmes.org
Since fused silica material possesses good mechanical properties, thermal and optical
properties, such as high hardness, low coefficient of thermal expansion, and wide …
properties, such as high hardness, low coefficient of thermal expansion, and wide …
Magnetorheological finishing for removing surface and subsurface defects of fused silica optics
R Catrin, J Neauport, D Taroux, P Cormont… - Optical …, 2014 - spiedigitallibrary.org
We investigate the capacity of magnetorheological finishing (MRF) process to remove
surface and subsurface defects of fused silica optics. Polished samples with engineered …
surface and subsurface defects of fused silica optics. Polished samples with engineered …