Recent advances in multi-functional coatings for soft magnetic composites
During the past 50 years, the aim to reduce the eddy current losses in magnetic cores to a
minimum led to the formulation of new materials starting from electrically insulated iron …
minimum led to the formulation of new materials starting from electrically insulated iron …
Investigation of magnetic properties, residual stress and densification in compacted iron powder specimens coated with polyepoxy
Soft magnetic powders are the main component of soft magnetic composites that are
covered by an insulation layer. In this work, iron powder with high purity is covered by an …
covered by an insulation layer. In this work, iron powder with high purity is covered by an …
Influence of particles size fraction on magnetic properties of soft magnetic composites prepared from a soft magnetic nanocrystalline powder with no synthetic oxide …
P Błyskun, M Kowalczyk, G Łukaszewicz… - Materials Science and …, 2021 - Elsevier
Soft magnetic composites (SMCs) are usually prepared from microcrystalline Fe, Fe-Si or Fe-
Si-Al powders. Other powders, including nanocrystalline ones, are relatively rarely used …
Si-Al powders. Other powders, including nanocrystalline ones, are relatively rarely used …
Rapid characterization method for SMC materials for a preliminary selection
In electrical machines, laminated steels are commonly adopted as soft magnetic materials,
while for permanent magnets, sintered ferrites and NdFeB are the most common solutions …
while for permanent magnets, sintered ferrites and NdFeB are the most common solutions …
Structural studies, magnetic properties and loss separation in iron–phenolicsilane soft magnetic composites
AH Taghvaei, H Shokrollahi, K Janghorban - Materials & Design, 2010 - Elsevier
In this work, six different series of iron based soft magnetic composites are produced and
studied:(1) passive iron powder;(2) passive iron powder-0.7% resin with coupling agent;(3) …
studied:(1) passive iron powder;(2) passive iron powder-0.7% resin with coupling agent;(3) …
Characteristics of power loss in soft magnetic composites a key for designing the best values of technological parameters
B Ślusarek, B Jankowski, K Sokalski… - Journal of Alloys and …, 2013 - Elsevier
In this paper, we consider a new way to choice values of technological parameters, such as
compaction pressure and hardening temperature which are required during preparation of …
compaction pressure and hardening temperature which are required during preparation of …
Steinmetz law in iron–phenolformaldehyde resin soft magnetic composites
P Kollár, V Vojtek, Z Birčáková, J Füzer… - Journal of magnetism …, 2014 - Elsevier
The validity of Steinmetz law describing the dc energy losses as a function of maximum
induction has been investigated for iron based soft magnetic composites (SMCs) up to 1.4 T …
induction has been investigated for iron based soft magnetic composites (SMCs) up to 1.4 T …
[HTML][HTML] Sintered powder cores of high Bs and low coreloss Fe84. 3Si4B8P3Cu0. 7 nano-crystalline alloy
Nano-crystalline Fe-rich Fe 84.3 Si 4 B 8 P 3 Cu 0.7 alloy ribbon with saturation magnetic
flux density (B s) close to Si-steel exhibits much lower core loss (W t) than Si-Steels. Low …
flux density (B s) close to Si-steel exhibits much lower core loss (W t) than Si-Steels. Low …
Wireless telemetry for instrumented component
DJ Mitchell, AA Kulkarni, R Subramanian… - US Patent …, 2013 - Google Patents
A telemetry system for use in a combustion turbine engine (10) having a compressor (12), a
combustor and a turbine (16) that includes a sensor (50, 74) in connection with a turbine …
combustor and a turbine (16) that includes a sensor (50, 74) in connection with a turbine …
Magnetic properties of amorphous Fe–Si–B powder cores mixed with pure iron powder
HJ Kim, SK Nam, KS Kim, SC Yoon… - Japanese Journal of …, 2012 - iopscience.iop.org
Abstract Amorphous Fe–Si–B alloy was prepared by melt-spinning, and then the ribbons
were pulverized and ball-milled to make the amorphous powder of∼ 25 µm in size …
were pulverized and ball-milled to make the amorphous powder of∼ 25 µm in size …