Effect of Lüders and Portevin–Le Chatelier localization bands on plasticity and fracture of notched steel specimens studied by DIC and FE simulations

SC Ren, TF Morgeneyer, M Mazière, S Forest… - International Journal of …, 2021 - Elsevier
The impact of the Portevin–Le Chatelier (PLC) effect on plasticity and fracture ahead of a
severe notch is investigated by DIC field measurements for C–Mn steel. The PLC effect …

[HTML][HTML] On the fatigue and dwell-fatigue behavior of a low-density steel and the correlated microstructure origin of damage mechanism

A Moshiri, A Zarei-Hanzaki, AS Anousheh… - journal of materials …, 2021 - Elsevier
The present work deals with revealing the fatigue and dwell-fatigue behavior and correlated
damage mechanisms of Fe–Mn–Al–C lightweight steel. Surprisingly, alteration in loading …

Low-cycle fatigue life and plasticity mechanisms of a Fe− 15Mn− 10Cr− 8Ni− 4Si seismic damping alloy under cyclic loading at various temperatures

T Sawaguchi, I Nikulin, K Ogawa, S Takamori… - Acta Materialia, 2021 - Elsevier
A recently developed Fe− 15Mn− 10Cr− 8Ni− 4Si (FMS) seismic damping alloy has a
superior fatigue life at room temperature due to reversible dislocation motion associated with …

The effect of preliminary creep-strain on material behavior under LCF tension/compression and pure torsion regimes

A Tomczyk, W Grodzki, A Seweryn - International Journal of Fatigue, 2024 - Elsevier
This paper presents the results of experimental tests of monotonic tension and torsion, creep-
rupture and preliminary creep at 200° C and 300° C, as well as low-cycle fatigue of …

[HTML][HTML] Hydrogen-assisted localized plasticity driven by dislocation pinning-depinning: Finite element simulations

D Sasaki, Y Kusaba, M Koyama - International Journal of Hydrogen Energy, 2024 - Elsevier
For the development of a hydrogen energy society, understanding hydrogen-assisted
fatigue crack propagation is crucial. Hydrogen-assisted fatigue crack propagation exhibits …

Dynamic strain aging behaviour in AISI 316L austenitic stainless steel under as-received and as-welded conditions

GA Muhamed, S Gündüz, MA Erden, D Taştemur - Metals, 2017 - mdpi.com
In the current study, dynamic strain ageing (DSA) phenomena in 316L austenitic stainless
steel was investigated under as-received and as-welded conditions. A tensile test was …

A review on the material development and corresponding properties for power plant applications

JP Patil, M Paliwal, SK Mishra - Materials …, 2022 - asmedigitalcollection.asme.org
Over the past decade, increased demand for energy generation at affordable rates and in a
clean state has been the driving force for material development for energy generation. In …

High-Temperature Low-Cycle Fatigue Behavior of HS80H Ferritic–Martensitic Steel Under Dynamic Strain Aging

W Wei, Y Feng, L Han, J Zhang, H Wang - Journal of Materials …, 2018 - Springer
In this work, low-cycle fatigue tests were performed on HS80H ferritic–martensitic steel with
the strain amplitudes ranging from 0.5 to 2.0% at room temperature and 350° C. The cyclic …

Strain-controlled fatigue and fracture of AISI 410 stainless steel

MJ Adinoyi, N Merah, J Albinmousa - Engineering Failure Analysis, 2019 - Elsevier
Microstructural characteristics, monotonic and strain-controlled cyclic axial behaviors of AISI
410 stainless steel were investigated. Grain size and distribution is uniform throughout the …

Effect of dynamic strain aging on cyclic deformation in piping material SA333 Gr-6 steel

G Kumar, A Kumar, HN Bar - International Journal of Pressure Vessels and …, 2021 - Elsevier
In piping structures, the low cycle fatigue loading arises from thermally induced strain cycles
associated with start-up and shut-downs and fluctuation in loading conditions. SA333 Gr-6 …