[HTML][HTML] Magnetic characterisation of microstructural feature distribution in P9 and T22 steels by major and minor BH loop measurements

J Liu, J Wilson, M Strangwood, CL Davis… - Journal of Magnetism and …, 2016 - Elsevier
This paper investigates the magnetic properties and parameters measured from major/minor
loops and used to characterise different microstructural feature distributions in P9 and T22 …

[HTML][HTML] Electromagnetic evaluation of the microstructure of Grade 91 tubes/pipes

J Liu, J Wilson, M Strangwood, CL Davis… - International Journal of …, 2015 - Elsevier
This paper assesses the feasibility of transferring a laboratory-based electromagnetic (EM)
sensor technique, which has already proved sensitive to significant (eg phase balance) or …

Continuous High-Temperature Thermoelectric Power Monitoring of Thermal Embrittlement

A Ruiz, B Lyons, H Granados-Becerra… - Journal of Nondestructive …, 2024 - Springer
Thermal embrittlement is a key concern for the structural integrity of engineering
components. Monitoring thermal embrittlement may indicate susceptibility to crack initiation …

Parametric description of power loss in soft magnetic materials with unbiased, rate-independent hysteresis loops

G Weir, J Leveneur, N Long - Journal of Magnetism and Magnetic Materials, 2022 - Elsevier
This paper develops a parametric model describing power loss per unit volume, PV, on
unbiased minor loops, in the low frequency limit, using the corresponding remanence B r …

Non-destructive characterisation of steel microstructures using electromagnetic sensors

L Zhou - 2015 - etheses.bham.ac.uk
Steel properties are controlled by its microstructural parameters, such as grain size, phase
balance and precipitates. It is desirable to monitor microstructural changes during …

Theory of low loss minor loops in soft magnetic composites

G Weir, W Trompetter, J Leveneur, N Long… - Journal of Magnetism …, 2023 - Elsevier
A theory of low loss, unbiased minor loops in an isothermal macroscopic composite of soft
magnetic particles is developed. The theory predicts an effective macroscopic shape factor …

Определение критических температур и структурного состояния 13%-ных хромистых сталей магнитометрическим методом

МЮ Беломытцев, ЕИ Кузько… - Известия высших …, 2017 - fermet.misis.ru
Аннотация В практике металловедения для анализа фазовых и структурных
превращений значительное применение находят методы, основанные на измерении …

[PDF][PDF] Creep monitoring using permanently installed potential drop sensors

J Corcoran - 2015 - core.ac.uk
Creep is the primary life limiting mechanism of static high temperature, high pressure power
station components. Creep state evaluation is currently achieved by surface inspection of …

[PDF][PDF] Magnetic NDT for steel microstructure characterisation–modelling the effect of ferrite grain size on magnetic properties

L Zhou, C Davis, P Kok, F Van Den Berg… - 19th World Conf. Non …, 2016 - ndt.net
The mechanical properties of steels are controlled by their microstructural parameters, such
as grain size, phase balance and precipitates, which are developed during thermo …

[PDF][PDF] Effects of thermal treatment on the mechanical and electromagnetic properties of 9Cr-1Mo steel

K Sodsai, M Noipitak, V Saetang… - Journal of Materials …, 2023 - academia.edu
This paper presents the effects of thermal treatment conditions on the mechanical properties