Hot corrosion and electrochemical behavior of NiCrAlY, NiCoCrAlY and NiCoCrAlYTa coatings in molten NaCl-Na2SO4 at 800° C
J Wang, D Li, T Shao - Surface and Coatings Technology, 2022 - Elsevier
Abstract The NiCrAlY, NiCoCrAlY and NiCoCrAlYTa coatings were prepared on a
Ni16Cr13Co4Mo alloy by the D-gun spray technique. The hot corrosion behaviors of the …
Ni16Cr13Co4Mo alloy by the D-gun spray technique. The hot corrosion behaviors of the …
Hot corrosion behavior of NiCr-Cr3C2-CaF2/BaF2 composite coating with NiAl bond coating in molten NaCl-KCl and NaCl-Na2SO4 at 800℃
JH Wang, DG Li, TM Shao - Corrosion Science, 2022 - Elsevier
Abstract The NiCr-Cr 3 C 2-CaF 2/BaF 2 coating with the NiAl bond coating was sprayed on
a Ni16Cr13Co4Mo (wt%) alloy by detonation-gun spray, and hot corrosion behaviors were …
a Ni16Cr13Co4Mo (wt%) alloy by detonation-gun spray, and hot corrosion behaviors were …
Effect of dynamic conditions on high-temperature corrosion of ternary carbonate salt for thermal energy storage applications
L González-Fernández, M Intxaurtieta-Carcedo… - Solar Energy Materials …, 2022 - Elsevier
Abstract Li 2 CO 3–Na 2 CO 3–K 2 CO 3 salt is one of the candidates for 3 rd generation
concentrated solar power (CSP) plants, aiming to increase the operational temperature. This …
concentrated solar power (CSP) plants, aiming to increase the operational temperature. This …
Corrosion mechanism of SS316L exposed to NaCl/Na2CO3 molten salt in air and argon environments
Molten salts are potential energy storage media for solar thermal power, but can be highly
corrosive. To investigate molten salt corrosion mechanisms, the oxidation state and structure …
corrosive. To investigate molten salt corrosion mechanisms, the oxidation state and structure …
Corrosion of iron–nickel–chromium alloys in high temperature carbonate salt under argon atmosphere
Next generation concentrated solar thermal power can produce receiver temperatures up to
800° C, however current solar salt based thermal storage is limited to 560° C. Eutectic salt …
800° C, however current solar salt based thermal storage is limited to 560° C. Eutectic salt …
Aggressive corrosion of C-276 nickel superalloy in chloride/sulphate eutectic salt
Molten salts are often used to store thermal energy in concentrating solar power plants. The
need for higher temperature thermal energy storage systems has prompted investigation …
need for higher temperature thermal energy storage systems has prompted investigation …
Corrosion resistance of 625 nickel superalloy exposed to isothermal and thermal cycling conditions in a chloride/carbonate salt
Using phase change materials as thermal energy storage media is a promising approach for
use in conjunction with concentrating solar thermal power (CSP)–particularly at the higher …
use in conjunction with concentrating solar thermal power (CSP)–particularly at the higher …
Early-stage corrosion of IN 740H alloy in eutectic NaCl-KCl molten salt at high temperatures
The next generation concentrated solar power plants are expected to operate at
temperatures above 700° C and this would necessitate heat storage media such as chloride …
temperatures above 700° C and this would necessitate heat storage media such as chloride …
C-276 nickel alloy corrosion in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions
Thermal energy storage (TES) is a key component for the practical application of
concentrating solar thermal power. Recently, a push for higher temperatures has increased …
concentrating solar thermal power. Recently, a push for higher temperatures has increased …
[HTML][HTML] Corrosion effects of Na2CO3/NaCl molten salt eutectic on 316L stainless steel under isothermal and cycling conditions
Using phase-change materials in thermal energy storage systems for concentrating solar
thermal plants can significantly reduce the volume of storage media and, therefore, the cost …
thermal plants can significantly reduce the volume of storage media and, therefore, the cost …