Recent developments in stainless steels
This article presents an overview of the developments in stainless steels made since the
1990s. Some of the new applications that involve the use of stainless steel are also …
1990s. Some of the new applications that involve the use of stainless steel are also …
S-phase surface engineering of Fe-Cr, Co-Cr and Ni-Cr alloys
H Dong - International Materials Reviews, 2010 - Taylor & Francis
Abstract Stainless steel, Co-Cr and Ni-Cr alloys have played an important role in many
industrial sectors to combat environmental degradation. However, low hardness and poor …
industrial sectors to combat environmental degradation. However, low hardness and poor …
Analysis of carbide transformation in MC-M23C6 and its effect on mechanical properties of Ni-based superalloy
X Song, Y Wang, X Zhao, J Zhang, Y Li, Y Wang… - Journal of Alloys and …, 2022 - Elsevier
An investigation based on electron microscopy and crystallographic analysis was employed
to gain insights into the carbide transformation in MC-M 23 C 6 complex carbide of …
to gain insights into the carbide transformation in MC-M 23 C 6 complex carbide of …
Tipping effect of tetra-alkylammonium on the potency of N-(6-(1H-benzo [d] imidazol-1-yl) hexyl)-N, N-dimethyldodecan-1-aminium bromide (BIDAB) as corrosion …
A new class of quaternary ammonium bromide; N-(6-(1H-benzo [d] imidazol-1-yl) hexyl)-N,
N-dimethyldodecan-1-aminium bromide (BIDAB) was successfully synthesized and …
N-dimethyldodecan-1-aminium bromide (BIDAB) was successfully synthesized and …
Corrosion behaviour of 316H stainless steel in molten FLiNaK eutectic salt containing graphite particles
The effect of various concentrations of graphite particles in molten FLiNaK eutectic salt (LiF-
NaF-KF: 46.5-11.5–42.0 mol.%) on the corrosion behaviour of 316H stainless steel was …
NaF-KF: 46.5-11.5–42.0 mol.%) on the corrosion behaviour of 316H stainless steel was …
Corrosion behavior of carburized 316 stainless steel in molten chloride salts
The corrosion has been investigated for carburized 316 stainless steel (SS) and 316SS in
ternary molten NaCl-KCl-MgCl 2 salt at 700° C under argon atmosphere when adding Mg …
ternary molten NaCl-KCl-MgCl 2 salt at 700° C under argon atmosphere when adding Mg …
The influence of stacking fault energy on plasticity mechanisms in triode-plasma nitrided austenitic stainless steels: Implications for the structure and stability of …
Austenitic stainless steels (ASSs), especially AISI type 304 and 316 ASSs, have been
extensively studied after thermochemical diffusion treatments (eg nitriding, carburising) to …
extensively studied after thermochemical diffusion treatments (eg nitriding, carburising) to …
Low-temperature carburization of austenitic stainless steels
SR Collins, PC Williams, SV Marx… - Heat Treating of …, 2014 - dl.asminternational.org
Low-temperature carburization hardens the surface of austenitic stainless steels through the
diffusion of interstitial carbon without the formation of carbides. This article provides an …
diffusion of interstitial carbon without the formation of carbides. This article provides an …
Microstructures and properties of roll-bonded stainless/medium carbon steel clad plates
Y Tao, J Yu-an, Y Xiaolin, L Wenbin, P Qihang… - Journal of Materials …, 2019 - Elsevier
A 304 stainless steel/medium carbon steel clad plate was fabricated by hot-rolling in an
argon atmosphere. The interfacial microstructures of the clad plates were observed by SEM …
argon atmosphere. The interfacial microstructures of the clad plates were observed by SEM …
Tribocorrosion behaviour of low temperature plasma carburised 316L stainless steel in 0.5 M NaCl solution
Experiments have been carried out to study the tribocorrosion behaviour of low temperature
plasma carburised 316L stainless steel under unidirectional sliding in 0.5 M NaCl solution …
plasma carburised 316L stainless steel under unidirectional sliding in 0.5 M NaCl solution …