Synergistic damage mechanisms of high-temperature metal corrosion in marine environments: A review
Y Liu, Y Zhou, W Wang, L Tian, J Zhao, J Sun - Progress in Organic …, 2024 - Elsevier
Marine equipment power systems often operate under high-temperature conditions, and
metal component corrosion in high-temperature environment can lead to failure of the entire …
metal component corrosion in high-temperature environment can lead to failure of the entire …
[HTML][HTML] Corrosion characteristics of 316L stainless steel in oxide-rich molten solar salt at 600° C
S Swaminathan, S Kumar, A Kranzmann… - Solar Energy Materials …, 2024 - Elsevier
An attempt has been made in this work, to observe the influence on alloy aging by the
sodium oxide (Na 2 O) in solar salt (60 wt% NaNO 3+ 40 wt% KNO 3). The accelerated …
sodium oxide (Na 2 O) in solar salt (60 wt% NaNO 3+ 40 wt% KNO 3). The accelerated …
[HTML][HTML] Corrosion effects of Na2CO3/NaCl molten salt eutectic on 316L stainless steel under isothermal and cycling conditions
Using phase-change materials in thermal energy storage systems for concentrating solar
thermal plants can significantly reduce the volume of storage media and, therefore, the cost …
thermal plants can significantly reduce the volume of storage media and, therefore, the cost …
Molecular dynamics study on interfacial diffusion characterization of nanoparticle TiO2 and metal Fe in high-temperature molten salt thermal energy storage system
X Yang, Z Guo, C Ji, Y Ma, J Xie - Solar Energy Materials and Solar Cells, 2024 - Elsevier
Previous experimental studies have found that nanoparticle TiO 2 doping into molten salts
can mitigate the corrosive effect of molten salts on metals; however, the microscopic …
can mitigate the corrosive effect of molten salts on metals; however, the microscopic …
Impact of CO32− impurities on the thermal performance of Solar Salt in thermal energy storage
Y Luo, P Song, X Yang, C Hu, Z Sun - Journal of Energy Storage, 2024 - Elsevier
Over the past decade, Solar Salt, composed of 60% NaNO 3 and 40% KNO 3, has emerged
as the optimal material for thermal energy storage (TES) in concentrating solar power (CSP) …
as the optimal material for thermal energy storage (TES) in concentrating solar power (CSP) …
High-temperature dynamic corrosion mechanisms of austenitic stainless and carbon steels in nitrates for concentrating solar power
P Yang, Z Deng, B Chen, Y Wang - Solar Energy Materials and Solar Cells, 2024 - Elsevier
Abstract: In this paper, to simulate the dynamic corrosion mechanisms of metals exposed to
a high-temperature molten salt mixture of NaNO 3–KNO 3, the experimental samples made …
a high-temperature molten salt mixture of NaNO 3–KNO 3, the experimental samples made …
Oxidation Kinetics of FeCr and FeCrAl Alloys: Influence of Secondary Processes
I Nakhutsrishvil - 2023 - preprints.org
The work presents a mathematical model of a thermogravimetric curve for the growth and
simultaneous sublimation of scale on a metal or alloy surface. Reduction of the reaction area …