Probability of growth of small damage sites on the exit surface of fused silica optics
RA Negres, GM Abdulla, DA Cross, ZM Liao… - Optics …, 2012 - opg.optica.org
Growth of laser damage on fused silica optical components depends on several key
parameters including laser fluence, wavelength, pulse duration, and site size. Here we …
parameters including laser fluence, wavelength, pulse duration, and site size. Here we …
Influence of bulk defects on bulk damage performance of fused silica optics at 355 nm nanosecond pulse laser
J Huang, H Liu, F Wang, X Ye, L Sun, X Zhou, Z Wu… - Optics …, 2017 - opg.optica.org
We demonstrate the effects of typical bulk defects in fused silica on the bulk damage
threshold under nanosecond UV pulse in this study. A new test method is proposed to …
threshold under nanosecond UV pulse in this study. A new test method is proposed to …
Time-resolved imaging of processes associated with exit-surface damage growth in fused silica following exposure to nanosecond laser pulses
SG Demos, RN Raman, RA Negres - Optics express, 2013 - opg.optica.org
We study the dynamics of energy deposition and subsequent material response associated
with exit surface damage growth in fused silica using a time resolved microscope system …
with exit surface damage growth in fused silica using a time resolved microscope system …
Quantitative identification of deposited energy in UV-transmitted KDP crystals from perspectives of electronic defects, atomic structure and sub-bandgap disturbance
The laser-induced damage threshold (LIDT) of ultra-precision machined potassium
dihydrogen phosphate (KDP) crystal is always lower than the intrinsic threshold. However …
dihydrogen phosphate (KDP) crystal is always lower than the intrinsic threshold. However …
Spatial sputtering of fused silica after a laser-induced exploding caused by a 355 nm nd: YAG laser
G Peng, P Zhang, Z Dong, J Chen, L Liang, C Zhu… - Frontiers in …, 2022 - frontiersin.org
To alleviate laser-induced threats in the high-power laser systems, it is necessary to
understand the debris propagation process and distribution characteristics, then take …
understand the debris propagation process and distribution characteristics, then take …
Exploration of the multiparameter space of nanosecond-laser damage growth in fused silica optics
RA Negres, ZM Liao, GM Abdulla, DA Cross… - Applied Optics, 2011 - opg.optica.org
Historically, the rate at which laser-induced damage sites grow on the exit surface of SiO_2
optics under subsequent illumination with nanosecond-laser pulses of any wavelength was …
optics under subsequent illumination with nanosecond-laser pulses of any wavelength was …
Self-focusing and stimulated Brillouin scattering effect of low-temporal coherence light and corresponding damage characteristics in fused silica
Laser-induced damage thresholds (LIDTs) of input/exit surfaces and filamentation of fused
silica under low-temporal coherence light (LTCL) and a corresponding damage mechanism …
silica under low-temporal coherence light (LTCL) and a corresponding damage mechanism …
Bulk damage growth characteristics and ultrafast diagnosis of fluoride-containing phosphate glasses induced by 355-nm laser
S Li, Y Jiang, R Wan, P Wang - Optics & Laser Technology, 2025 - Elsevier
To comprehensively reveal the influence regularity of different glass melting temperatures
on the ultraviolet (UV) laser-induced damage resistance of fluoride-containing phosphate …
on the ultraviolet (UV) laser-induced damage resistance of fluoride-containing phosphate …
[HTML][HTML] Accumulated self-focusing of ultraviolet light in silica glass
R Khrapko, C Lai, J Casey, WA Wood… - Applied Physics …, 2014 - pubs.aip.org
Exposure to UV light induces structural changes in silica glass. This leads to a change in
density, refractive index, optical absorption, and stress. Prolonged exposure causes …
density, refractive index, optical absorption, and stress. Prolonged exposure causes …
Filamentation and surface damage in fused silica with single-mode and multi-mode pulses
H Bercegol, L Lamaignère, V Cavaro… - … -Induced Damage in …, 2006 - spiedigitallibrary.org
We studied filamentation, front surface damage and rear surface damage at 1064 nm and
351 nm with nanosecond pulses on a fused silica optical window. With temporally single …
351 nm with nanosecond pulses on a fused silica optical window. With temporally single …