Cellular/dendritic arrays and intermetallic phases affecting corrosion and mechanical resistances of an Al–Mg–Si alloy
Abstract Outdoor applications of Al–Mg–Si alloys have been specified due to their very good
corrosion resistance when compared with those of other aluminum alloys. Nevertheless …
corrosion resistance when compared with those of other aluminum alloys. Nevertheless …
Influence of heat-treatment cycles on the microstructure, mechanical properties, and corrosion resistance of co-cr dental alloys fabricated by selective laser melting
The effect of repeated heat-treatment (HT) cycles, as precisely applied in the regular dental
practice to produce metal-ceramic restorations, on microstructure, mechanical properties …
practice to produce metal-ceramic restorations, on microstructure, mechanical properties …
[HTML][HTML] Effect of holding time, thickness and heat treatment on microstructure and mechanical properties of compacted graphite cast iron
H Megahed, E El-Kashif, AY Shash… - Journal of Materials …, 2019 - Elsevier
The effect of holding time, thickness and annealing heat treatment on the microstructure and
some mechanical properties of compacted graphite iron (CGI) are studied. Samples of CGI …
some mechanical properties of compacted graphite iron (CGI) are studied. Samples of CGI …
Corrosion performance and degradation mechanism of a bi-metallic aluminum structure processed by wire-arc additive manufacturing
Abstract An Al-5Mg alloy (AA5083) block, deposited over an AA6061 substrate by wire-arc
additive manufacturing, was electrochemically tested along two different cross-sectional …
additive manufacturing, was electrochemically tested along two different cross-sectional …
Effect of sintering time on corrosion behavior of an Ag/Al/Nb/Ti/Zn alloy system
High-entropy alloys are interesting for both aerospace and biomedical applications.
Additionally, their application into a corrosive environment is also demanded. Investigations …
Additionally, their application into a corrosive environment is also demanded. Investigations …
Corrosion behavior of an Al-Si casting and a sintered Al/Si composite immersed into biodiesel and blends
ALP Elias, MS Koizumi, EL Ortiz, JFQ Rodrigues… - Fuel processing …, 2020 - Elsevier
This investigation is focused on the corrosion evaluation of an as-cast Al-7.5 wt% Si alloy
and an Al/7.5 wt% Si composite immersed into distinctive biofuels. Immersions up to~ 6000 …
and an Al/7.5 wt% Si composite immersed into distinctive biofuels. Immersions up to~ 6000 …
[HTML][HTML] Corrosion behavior of Al-15% Mg2Si alloy with 1% Ni addition
Y Sun, C Li, L Yu, Z Gao, X Xia, Y Liu - Results in Physics, 2020 - Elsevier
Abstract Corrosion behaviors of Al-15% Mg 2 Si-1% Ni alloy in 3.5% NaCl solution were
studied by characterizing the corrosion morphologies of Al 3 Ni, Mg 2 Si, and Al phases. The …
studied by characterizing the corrosion morphologies of Al 3 Ni, Mg 2 Si, and Al phases. The …
Electrochemical and corrosion study of as-cast NixAly intermetallic alloys: Influence of alloy composition and electrolyte pH
B Sefer, S Virtanen - Corrosion Science, 2019 - Elsevier
Electrochemical and corrosion behaviour of as-cast NixAly intermetallic alloys (Ni25Al75,
Ni40Al60, Ni50Al50 and Ni75Al25 in at.%) is investigated and compared with commercially …
Ni40Al60, Ni50Al50 and Ni75Al25 in at.%) is investigated and compared with commercially …
Effects of in situ intermetallics on the microstructural array and saline corrosion performance of cast Al/WCp composites
AG Lekatou, N Gkikas, V Gousia, K Lentzaris… - Journal of Materials …, 2018 - Springer
Al-matrix composites, ex situ reinforced with WC nanoparticles and in situ reinforced with Al
3 (Ti, W), Al 12 W, Al 5 W and Al 4 W, have been fabricated by casting assisted by K 2 TiF 6 …
3 (Ti, W), Al 12 W, Al 5 W and Al 4 W, have been fabricated by casting assisted by K 2 TiF 6 …
Corrosion behavior of 2099 Al–Li alloy in NaCl aqueous solution
B Chen, CH Li, SC He, X Li, C Lu - Journal of Materials Research, 2014 - cambridge.org
The corrosion behavior of 2099 Al–Li alloy in NaCl aqueous solutions with different
concentrations (1.5, 3.5, and 5.0% in mass fraction) was investigated. Its corrosion …
concentrations (1.5, 3.5, and 5.0% in mass fraction) was investigated. Its corrosion …