Mechanical behaviour of Zn–Al–Cu–Mg alloys: Deformation mechanisms of as-cast microstructures

Z Wu, S Sandlöbes, L Wu, W Hu, G Gottstein… - Materials Science and …, 2016 - Elsevier
We study the effects of dilute Mg addition on the microstructure formation and mechanical
properties of a ZnAl4Cu1 alloy. On the basis of the composition of the commercial alloy Z410 …

The effect of manganese on the microstructure and mechanical properties of zinc–aluminium based ZA-8 alloy

A Türk, M Durman, ES Kayali - Journal of materials science, 2007 - Springer
In this investigation, the effect of manganese as an alloying element in the range 0.01%–
0.53 wt.%, on the hardness, 0.2% yield, tensile and impact strength, and creep properties of …

Effect of severe plastic deformation on tensile properties and impact toughness of two-phase Zn–40Al alloy

G Purcek, O Saray, I Karaman… - Materials Science and …, 2008 - Elsevier
Tensile properties and impact toughness of the severe plastically deformed Zn–40Al alloy
were investigated. The material billets were subjected to equal-channel angular extrusion …

Effects of electrolytes on the growth behavior, microstructure and tribological properties of plasma electrolytic oxidation coatings on a ZA27 alloy

G Bian, L Wang, J Wu, J Zheng, H Sun… - Surface and Coatings …, 2015 - Elsevier
In this study, plasma electrolytic oxidation (PEO) was successfully applied on a ZA27 alloy to
produce continuous and dense ceramic coatings. The effects of the electrolytes (silicate …

Tribological and corrosion properties of coatings produced by plasma electrolytic oxidation on the ZA27 alloy

G Li, Y Mao, Z Li, L Wang, H DaCosta - Journal of Materials Engineering …, 2018 - Springer
In this paper, a continuous and dense coating was deposited on samples of the ZA27 alloy
through the plasma electrolytic oxidation (PEO) process to improve its wear and corrosion …

Enhancement in mechanical behavior and wear resistance of severe plastically deformed two-phase Zn–Al alloys

G Purcek, I Karaman, GG Yapici… - International journal of …, 2007 - degruyter.com
The microstructural evolution, tensile response and wear properties of a two-phase Zn–Al
alloy (Zn-8 wt.% Al, ZA-8) have been studied after severe plastic deformation by equal …

Flow response of a severe plastically deformed two-phase zinc–aluminum alloy

M Al-Maharbi, I Karaman, G Purcek - Materials Science and Engineering: A, 2010 - Elsevier
A two-phase zinc–aluminum alloy (Zn–8wt.% Al) has been subjected to severe plastic
deformation via equal channel angular extrusion (ECAE). The alloy was successfully …

The Effect of Ti–B and Sr on the mechanical behaviour of the Zinc–Aluminum-based ZA-12 alloy produced by gravity casting

S Can Kurnaz, H Sevik, A Türk… - International journal of …, 2022 - degruyter.com
In this study, the effect of Ti–B (0.05–0.7 wt.% Ti, 0.01–0.13 wt.% B) and Sr additions (0.05–
0.7 wt.%) on the hardness, ultimate tensile strength (UTS), strain and fatigue properties of …

Microstructure and creep behaviour of Zn-10Al alloy with V additives at ambient temperature

X Liu, G Lin, M Chen - Materials Letters, 2022 - Elsevier
The effect of V alloying on the creep properties of the Zn-10Al alloy at ambient temperature
was investigated. V alloying significantly refined the Zn-10Al grains, and a new Al 3 V phase …

[图书][B] Mechanical flow response and anisotropy in ultra-fine grained magnesium and zinc alloys

M Al Maharbi - 2009 - search.proquest.com
Hexagonal closed packed (hcp) materials, in contrast to cubic materials, possess several