Ni-W electrodeposited coatings: Characterization, properties and applications
MH Allahyarzadeh, M Aliofkhazraei… - Surface and Coatings …, 2016 - Elsevier
Nowadays, application of nanocrystalline nickel-tungsten (Ni-W) alloys is receiving a great
interest because they are an efficient replacement for hard chromium coatings owing to their …
interest because they are an efficient replacement for hard chromium coatings owing to their …
A review of fatigue behavior in nanocrystalline metals
HA Padilla, BL Boyce - Experimental mechanics, 2010 - Springer
Nanocrystalline metals have been shown to exhibit unique mechanical behavior, including
break-down in Hall-Petch behavior, suppression of dislocation-mediated plasticity, induction …
break-down in Hall-Petch behavior, suppression of dislocation-mediated plasticity, induction …
Corrosion of nanocrystalline Ni–W alloys in alkaline and acidic 3.5 wt.% NaCl solutions
A Chianpairot, G Lothongkum, CA Schuh… - Corrosion …, 2011 - Elsevier
The corrosion behaviour of reverse-pulse electrodeposited nanocrystalline nickel tungsten
alloys (nc Ni–W) in pH 3 and 10 3.5 wt.% NaCl solutions is investigated and analysed as a …
alloys (nc Ni–W) in pH 3 and 10 3.5 wt.% NaCl solutions is investigated and analysed as a …
Stress-sensitive fatigue crack initiation mechanisms of coated titanium alloy
The presence of hard coatings can reduce the fatigue life of metal substrates to an
unacceptable level, causing the catastrophic failure of load-bearing structures …
unacceptable level, causing the catastrophic failure of load-bearing structures …
Novel antibacterial biodegradable Fe-Mn-Ag alloys produced by mechanical alloying
Various compositions and synthesis methods of biodegradable iron-based alloys have been
studied aiming for the use of temporary medical implants. However, none is focused on …
studied aiming for the use of temporary medical implants. However, none is focused on …
Friction and sliding wear behaviour of electrodeposited cobalt and cobalt–tungsten alloy coatings for replacement of electrodeposited chromium
DP Weston, PH Shipway, SJ Harris, MK Cheng - Wear, 2009 - Elsevier
Electroplated chromium coatings have been widely used in the automotive, aerospace,
manufacturing industries for applications such as internal combustion engine components …
manufacturing industries for applications such as internal combustion engine components …
A review on the corrosion fatigue strength of surface-modified stainless steels
Materials are often exposed to simultaneous actions of corrosive environment and repeated
stress, which sometimes leads to a significant decrease in corrosion fatigue strength …
stress, which sometimes leads to a significant decrease in corrosion fatigue strength …
[HTML][HTML] Fabrication of permanent self-lubricating 2D material-reinforced nickel mould tools using electroforming
In the replication of polymeric micro/nano structures, adhesion and friction between mould
tool and polymer cause significant feature failure. For the first time, this work developed a …
tool and polymer cause significant feature failure. For the first time, this work developed a …
Corrosion, oxidation and wear study of electro-co-deposited ZrO2-TiO2 reinforced Ni-W coatings
S Shajahan, A Basu - Surface and Coatings Technology, 2020 - Elsevier
The pulsed electro-co-deposition process was used on mild steel substrate to develop Ni-W
based composite coating which comprises of ZrO 2 and TiO 2 oxide nanoparticles. In the …
based composite coating which comprises of ZrO 2 and TiO 2 oxide nanoparticles. In the …
Regulation of enamel hardness by its crystallographic dimensions
Enamel is a composite biomaterial comprising a minor organic matrix (∼ 2%) and a
hierarchically organized inorganic ultrastructure (∼ 96–98%). Surprisingly, to date there is …
hierarchically organized inorganic ultrastructure (∼ 96–98%). Surprisingly, to date there is …