Weathering steels: From empirical development to scientific design. A review
M Morcillo, I Díaz, B Chico, H Cano, D De la Fuente - Corrosion Science, 2014 - Elsevier
The design of the first weathering steels was purely empirical and focused on a small
number of conventional alloying elements such as manganese, silicon, chromium, nickel …
number of conventional alloying elements such as manganese, silicon, chromium, nickel …
Atmospheric corrosion of weathering steels. Overview for engineers. Part II: Testing, inspection, maintenance
M Morcillo, I Díaz, H Cano, B Chico… - … and Building Materials, 2019 - Elsevier
The atmospheric corrosion of weathering steel (WS) has been extensively discussed in the
scientific literature, but a comprehensive overview of this topic from an engineering …
scientific literature, but a comprehensive overview of this topic from an engineering …
Fundamental understanding on the effect of Cr on corrosion resistance of weathering steel in simulated tropical marine atmosphere
M Sun, C Du, Z Liu, C Liu, X Li, Y Wu - Corrosion science, 2021 - Elsevier
The role of Cr on the corrosion resistance of weathering steel in simulated tropical marine
atmosphere was investigated by the dry/wet cyclic corrosion test. The addition of Cr in steel …
atmosphere was investigated by the dry/wet cyclic corrosion test. The addition of Cr in steel …
Synergy of Cu and Sb to enhance the resistance of 3% Ni weathering steel to marine atmospheric corrosion
Various contents of Cu and Sb elements were incorporated into 3% Ni steel to enhance its
corrosion resistance in a simulated tropical marine atmosphere of high salinity. The …
corrosion resistance in a simulated tropical marine atmosphere of high salinity. The …
Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in Maldives
Corrosion product film (CPF) formation and its beneficial effect on corrosion protection of a
Ni advanced weathering steel (WS), 3Ni WS, was investigated under the harsh marine …
Ni advanced weathering steel (WS), 3Ni WS, was investigated under the harsh marine …
Clarifying the effect of a small amount of Cr content on the corrosion of Ni-Mo steel in tropical marine atmospheric environment
B Dong, W Liu, T Zhang, L Chen, Y Fan, Y Zhao, H Li… - Corrosion …, 2023 - Elsevier
The effect of Cr content on the corrosion behavior of Ni-Mo steel in the tropical marine
atmospheric environment is systematically investigated. The increase of Cr content …
atmospheric environment is systematically investigated. The increase of Cr content …
Unraveling the effect of chloride ion on the corrosion product film of Cr-Ni-containing steel in tropical marine atmospheric environment
B Dong, W Liu, L Chen, T Zhang, Y Fan, Y Zhao, H Li… - Corrosion …, 2022 - Elsevier
The effect of Cl-concentration on the corrosion behavior of Cr-containing steel in tropical
marine atmospheric environment is systematically studied. Cl-ions affect the adsorption …
marine atmospheric environment is systematically studied. Cl-ions affect the adsorption …
Corrosion failure analysis of low alloy steel and carbon steel rebar in tropical marine atmospheric environment: Outdoor exposure and indoor test
B Dong, W Liu, T Zhang, L Chen, Y Fan, Y Zhao… - Engineering Failure …, 2021 - Elsevier
Carbon steel rebar seriously corrodes in severe tropical marine atmospheric environment,
threatening the safety of building structures. Hence, it is of great significance to design and …
threatening the safety of building structures. Hence, it is of great significance to design and …
Insight into the product film formed on Ni-advanced weathering steel in a tropical marine atmosphere
The product film formed on Ni-advanced weathering steel in a tropical marine environment
was investigated in detail through outdoor exposure by using diverse surface analysis …
was investigated in detail through outdoor exposure by using diverse surface analysis …
Atmospheric corrosion of Ni-advanced weathering steels in marine atmospheres of moderate salinity
One conventional and three Ni-advanced weathering steels have been exposed for one
year in two marine atmospheres of moderate aggressivity (30 and 75 mg Cl−/m 2 d). The …
year in two marine atmospheres of moderate aggressivity (30 and 75 mg Cl−/m 2 d). The …