A review on the properties of iron aluminide intermetallics

M Zamanzade, A Barnoush, C Motz - Crystals, 2016 - mdpi.com
Iron aluminides have been among the most studied intermetallics since the 1930s, when
their excellent oxidation resistance was first noticed. Their low cost of production, low …

Reversible hydrogen trapping in a 3.5 NiCrMoV medium strength steel

Q Liu, A Atrens - Corrosion Science, 2015 - Elsevier
Reversible hydrogen trapping was investigated in a 3.5 NiCrMoV quenched and tempered
martensitic steel by means of hydrogen permeation experiments. The lattice diffusion …

Determination of trapping parameters and the chemical diffusion coefficient from hydrogen permeation experiments

J Svoboda, G Mori, A Prethaler, FD Fischer - Corrosion Science, 2014 - Elsevier
An improved diffusion theory accounting for trapping effects is applied to evaluation of
hydrogen permeation experiments performed for pure iron and pearlitic and martensitic …

Modelling the influence of trapping on hydrogen permeation in metals

FD Fischer, G Mori, J Svoboda - Corrosion science, 2013 - Elsevier
Hydrogen permeation (diffusion) is strongly influenced by the local hydrogen concentration
and by the density and depth of traps. Consequently hydrogen diffusion cannot be described …

Cr effect on hydrogen embrittlement of Fe3Al-based iron aluminide intermetallics: Surface or bulk effect

M Zamanzade, H Vehoff, A Barnoush - Acta materialia, 2014 - Elsevier
The objective of this work is to reduce the susceptibility of binary Fe 3 Al intermetallics to
hydrogen embrittlement with the addition of chromium as the ternary element. The Young's …

Enhanced inhibition on hydrogen permeation during electrodeposition process by rare earth (RE= Ce) salt additive

P Zhang, Z Xu, B Zhang, B Lei, Z Feng, G Meng… - International Journal of …, 2022 - Elsevier
High-strength steel parts are electroplated with corrosion-resistant coatings and then
subjected to hydrogen removal annealing to prevent hydrogen embrittlement. This approach …

Effects of hydrogen on the anodic behavior of Alloy 690 at 60 C

T Dan, T Shoji, Z Lu, K Sakaguchi, J Wang, EH Han… - Corrosion …, 2010 - Elsevier
Polarization and electrochemical impedance spectroscopy (EIS) measurements, Mott–
Schottky (M–S) analysis and X-ray photoelectron spectroscopy (XPS) were used to …

First-principles assessment of hydrogen absorption into FeAl and Fe3Si: Towards prevention of steel embrittlement

DF Johnson, EA Carter - Acta Materialia, 2010 - Elsevier
We characterize the ability of two potential surface alloys, FeAl and Fe3Si, to prevent H
incorporation into steel, with a view toward inhibiting steel embrittlement. Periodic density …

Effect of electrodeposition parameters on the hydrogen permeation during Cu–Sn alloy electrodeposition

G Meng, F Sun, S Wang, Y Shao, T Zhang, F Wang - Electrochimica Acta, 2010 - Elsevier
The Cu–Sn alloy coatings were synthesized on 27SiMn steel by direct current (DC), pulse
current (PC) and pulse reverse current (PRC) electrodeposition techniques from …

[HTML][HTML] A better understanding of hydrogen trapping and diffusion in aluminized press-hardenable steels

M Krid, M Mandy, T Sturel, R Grigorieva, P Drillet… - Journal of Materials …, 2024 - Elsevier
Press hardenable steels (PHS) coated with Al–Si alloy are widely used in the automotive
industry owing to their good mechanical properties (Yield Strength> 1200 MPa and Tensile …