Mechanical strength predictability of full factorial, Taguchi, and Box Behnken designs: Optimization of thermal settings and Cellulose Nanofibers content in PA12 for …
Optimization of reinforced nanocomposites for MEX 3D-printing remain strong industrial
claims. Herein, the efficacy of three modeling methods, ie, full factorial (FFD), Taguchi (TD) …
claims. Herein, the efficacy of three modeling methods, ie, full factorial (FFD), Taguchi (TD) …
[HTML][HTML] Effects of Laser Power and Hatch Orientation on Final Properties of PA12 Parts Produced by Selective Laser Sintering
Poly (dodecano-12-lactam)(commercially known as polyamide “PA12”) is one of the most
resourceful materials used in the selective laser sintering (SLS) process due to its chemical …
resourceful materials used in the selective laser sintering (SLS) process due to its chemical …
Tensile strength and wear resistance of glass-reinforced PA1212 fabricated by selective laser sintering
T Wu, Y Ren, L Liang, J Wen, H Wu, Y Tian… - Virtual and Physical …, 2023 - Taylor & Francis
Glass fibre (GF) and glass bead (GB)–reinforced polyamide1212 (PA1212) was additively
manufactured by selective laser sintering. The effects of laser power and GF content on the …
manufactured by selective laser sintering. The effects of laser power and GF content on the …
[HTML][HTML] Tribological properties of glass bead-filled polyamide 12 composite manufactured by selective laser sintering
A Gadelmoula, SA Aldahash - Polymers, 2023 - mdpi.com
To enhance the properties of polyamide 12 (PA12/Nylon 12) manufactured by the selective
laser sintering (SLS) process, micron-sized glass beads are used as a filler, and the …
laser sintering (SLS) process, micron-sized glass beads are used as a filler, and the …
[HTML][HTML] Possibilities of a Hybrid Method for a Time-Scale-Frequency Analysis in the Aspect of Identifying Surface Topography Irregularities
The article presents research results related to assessing the possibilities of applying
modern filtration methods to diagnosing measurement signals. The Fourier transformation …
modern filtration methods to diagnosing measurement signals. The Fourier transformation …
[HTML][HTML] Dry Friction and Wear Behavior of Laser-Sintered Graphite/Carbon Fiber/Polyamide 12 Composite
A Gadelmoula, SA Aldahash - Polymers, 2023 - mdpi.com
Carbon fiber-reinforced polymers (CFRPs) are being used extensively in modern industries
that require a high strength-to-weight ratio, such as aerospace, automotive, motorsport, and …
that require a high strength-to-weight ratio, such as aerospace, automotive, motorsport, and …
[HTML][HTML] Influence of Build Orientation and Part Thickness on Tensile Properties of Polyamide 12 Parts Manufactured by Selective Laser Sintering
JJ Slager, BC Earp, AM Ibrahim - Polymers, 2024 - mdpi.com
The use of additive manufacturing to rapidly test and evaluate solutions to engineering
problems has been demonstrated. Selective laser sintering (SLS) is a subset of additive …
problems has been demonstrated. Selective laser sintering (SLS) is a subset of additive …
[HTML][HTML] Effect of PA12 powder recycling on properties of SLS 3D printed parts including their hygroscopicity
The ageing and recycling of polyamide 12 (PA12) powder are key issues in selective laser
sintering (SLS) processing, while hygroscopicity is an important defect of PA12 products …
sintering (SLS) processing, while hygroscopicity is an important defect of PA12 products …
[HTML][HTML] Multiscale data treatment in additive manufacturing
D Gogolewski - Materials, 2023 - mdpi.com
The article assesses the impact of data treatment on the possibility of assessing the
morphological features of additively manufactured spherical surfaces. Tests were carried out …
morphological features of additively manufactured spherical surfaces. Tests were carried out …
Investigation of the ageing conditions of PEEK powder for the selective laser sintering process
Y Guo, H Chen, S Tian, Y Xu, K Ma, S Ma… - Virtual and Physical …, 2023 - Taylor & Francis
Ageing mechanism of PEEK powders at optimal powder bed temperature (T b) and factors
affecting their reusability remain unclear. This study investigated effects of gas type (air …
affecting their reusability remain unclear. This study investigated effects of gas type (air …