[HTML][HTML] Numerical and thermal analysis of mechanical properties degradations and distortions in steel weld joint
JL Chukwuneke, MI Ndefo, JE Sinebe, SM Ofochebe - Cleaner Materials, 2022 - Elsevier
To quantify the degradation of mechanical properties and material distortion associated with
steel weld. Twin mild steel plates each of dimension 20 mm× 100 mm× 6 mm were joined in …
steel weld. Twin mild steel plates each of dimension 20 mm× 100 mm× 6 mm were joined in …
Electrochemical characterization of steel bridge welds under simulated durability test
Ever increasingly, corrosion-induced steel bridge deterioration, particularly near or at the
welded joints, has led to a huge economic burden in the United States. There is, however …
welded joints, has led to a huge economic burden in the United States. There is, however …
[PDF][PDF] Change of mechanical properties of zinc coatings after heat treatment
J Votava, V Kumbár, A Polcar, M Fajman - Acta Technologica …, 2020 - sciendo.com
Hot-dip galvanized coatings represent a protection based on passivation of the single zinc
layer. It is one of the most commonly used surface treatments of steel. However, pure zinc …
layer. It is one of the most commonly used surface treatments of steel. However, pure zinc …
Usage of abrasion-resistant materials in agriculture
J Votava - Journal of Central European Agriculture, 2014 - hrcak.srce.hr
Agricultural soil-processing machines are subject to an extensive abrasive wear. This paper
analyses technical materials and their fitness to exchangeable parts of plough bottoms, such …
analyses technical materials and their fitness to exchangeable parts of plough bottoms, such …
Impact of insufficient cleaning on the quality of molybdenum layer applied by thermal spraying
M Bujna, M Prístavka, P Kaplík - Advanced Materials Research, 2013 - Trans Tech Publ
Thermal spraying influences several physical and chemical properties of the coating
surface. The most important of them are hardness, density, porosity, corrosion resistance …
surface. The most important of them are hardness, density, porosity, corrosion resistance …
[PDF][PDF] Degradation processes in anticorrosive coatings for machinery designed for fertiliser application.
J Votava, V Kumbár, A Polcar - Acta Universitatis Agriculturae et …, 2016 - acta.mendelu.cz
In agricultural practice, anticorrosion protection of steel components is utterly indispensable.
It is of particular importance for machines and devices working in an environment with …
It is of particular importance for machines and devices working in an environment with …
PEMBUATAN DAN PENGUJIAN SIFAT MEKANIK WELDING SPESIMEN LOGAM DISSIMILAR AISI 1015 DENGAN AISI 304L MENGGUNAKAN PROSES GMAW
R Riswanda, H Kadir, A Saragih - Jurnal Rekayasa Mesin, 2024 - rekayasamesin.ub.ac.id
2.2. Methods Proses pengelasan seperti pada gambar 1 dilakukan secara manual dengan
polaritas arus las DCRP (Direct Current Reverse Polarity). Pengelasan dilakukan pada …
polaritas arus las DCRP (Direct Current Reverse Polarity). Pengelasan dilakukan pada …
[PDF][PDF] Application of hard metal weld deposit in the area of mixing organic materials
J Votava, V Kumbár - Acta Universitatis Agriculturae et …, 2014 - researchgate.net
APPLICATION OF HARD METAL WELD DEPOSIT IN THE AREA OF MIXING ORGANIC
MATERIALS Page 1 1161 ACTA UNIVERSITATIS AGRICULTURAE ET SILVICULTURAE …
MATERIALS Page 1 1161 ACTA UNIVERSITATIS AGRICULTURAE ET SILVICULTURAE …
[HTML][HTML] Influence of roughness on quality molybdenum deposit layer by thermal spraying
In this paper we deal with the impact of roughness on the quality of molybdenum layer.
Insufficient cleaning may result in a poor quality of the sprayed layer. Our aim is to analyze …
Insufficient cleaning may result in a poor quality of the sprayed layer. Our aim is to analyze …
[PDF][PDF] Cleaner Materials
JL Chukwuneke, MI Ndefo, JE Sinebe, SM Ofochebe - researchgate.net
To quantify the degradation of mechanical properties and material distortion associated with
steel weld. Twin mild steel plates each of dimension 20 mm× 100 mm× 6 mm were joined in …
steel weld. Twin mild steel plates each of dimension 20 mm× 100 mm× 6 mm were joined in …