Assessment of the factors influencing micropitting in rolling/sliding contacts
Micropitting is currently a significant failure mechanism in carburised steel gears, but the
detailed mechanisms of crack initiation and propagation are not well understood …
detailed mechanisms of crack initiation and propagation are not well understood …
[HTML][HTML] Running-in and micropitting behaviour of steel surfaces under mixed lubrication conditions
A Clarke, IJJ Weeks, RW Snidle, HP Evans - Tribology International, 2016 - Elsevier
The paper investigates the running-in of hardened steel surfaces under mixed lubrication
conditions. Pairs of surfaces of both equal and differing hardness were loaded together …
conditions. Pairs of surfaces of both equal and differing hardness were loaded together …
Contact fatigue performance of helical gears with surface coatings
The objective of this study was to evaluate the performance of helical gears with applied
surface coatings either with or without Inorganic Fullerence Like Material (IFLM) nano …
surface coatings either with or without Inorganic Fullerence Like Material (IFLM) nano …
Martensite decay in micropitted gears
Metallographic examination performed on a number of micropitted gears has revealed
microstructural features similar to those reported in the literature in fatigued bearings …
microstructural features similar to those reported in the literature in fatigued bearings …
An observation on the initiation of micro-pitting damage in as-ground and coated gears during contact fatigue
The effect of surface features on as-ground gears and the influence of BALINIT® C and Nb–
S coatings on the initiation of micro-pitting damage have been examined in case-carburised …
S coatings on the initiation of micro-pitting damage have been examined in case-carburised …
Assessment of topography parameters during running-in and subsequent rolling contact fatigue tests
DK Prajapati, M Tiwari - Journal of Tribology, 2019 - asmedigitalcollection.asme.org
Rolling contact fatigue (RCF) is one of the major problems observed in gear mechanisms,
which leads to high friction, ultimately resulting in high energy consumption. This paper …
which leads to high friction, ultimately resulting in high energy consumption. This paper …
Effect of as-ground surface and the BALINIT® C and Nb–S coatings on contact fatigue damage in gears
The influence of as-ground surface and the BALINIT® C and Nb–S coatings on contact
fatigue damage have been investigated using testing of case-carburised S156 steel helical …
fatigue damage have been investigated using testing of case-carburised S156 steel helical …
Elastic properties of eta carbide (η-Fe2C) from ab initio calculations: application to cryogenically treated gear steel
The elastic properties of η-Fe _2 C η-Fe 2 C (eta carbide) have been determined from ab
initio density functional theory calculations using the generalized gradient approximation …
initio density functional theory calculations using the generalized gradient approximation …
Zuverlässige Beurteilung der Zahnrad-Graufleckentragfähigkeit von Getriebeölen
NL Sagraloff - 2022 - mediatum.ub.tum.de
Durch Einsatz von Getriebeölen mit einer hohen Graufleckentragfähigkeit, kann der
kostspielige Tausch von betroffenen Zahnrädern vermieden werden. Daher müssen Öle …
kostspielige Tausch von betroffenen Zahnrädern vermieden werden. Daher müssen Öle …
[PDF][PDF] Effects of Variable Load and Rotational Speed Conditions on Gear Micropitting in Wind Turbine Gearboxes
I Al Tubi - 2014 - etheses.whiterose.ac.uk
Micropitting damage is one of the failure modes commonly observed on gears and bearings
in wind turbine (WT) gearboxes. It can lead to destructive failures which, in turn, lead to …
in wind turbine (WT) gearboxes. It can lead to destructive failures which, in turn, lead to …