Indentation testing and its acoustic emission response: applications and emerging trends

NH Faisal, R Ahmed… - International Materials …, 2011 - journals.sagepub.com
This review summarises the state of knowledge on acoustic emission (AE) techniques
applied to material property evaluation during indentation (eg hardness) testing. There are …

Effect of mechanical properties of CrN/CrCN coatings and uncoated 1.402 stainless steel on the evolution of degradation and surface roughness in cavitation erosion

A Krella, A Marchewicz - Tribology International, 2023 - Elsevier
The effect of the mechanical properties of CrN/CrCN multilayer ceramic coatings on
cavitation degradation and surface roughness was investigated. Three coatings with …

Study on self-loosening of bolted joints excited by dynamic axial load

J Liu, H Ouyang, Z Feng, Z Cai, X Liu, M Zhu - Tribology international, 2017 - Elsevier
Loosening tests of bolted joints are carried out under various preloads and excitation
amplitudes. Three coatings are utilized to treat bolts, and their effects on the anti-loosening …

Designing superhard, self-toughening CrAlN coatings through grain boundary engineering

Z Li, P Munroe, Z Jiang, X Zhao, J Xu, Z Zhou, J Jiang… - Acta Materialia, 2012 - Elsevier
One of the toughest challenges that hinders the application of ceramic coatings is their poor
damage tolerance. Addressing this problem requires the development of novel micro-or …

Evaluation of the surface fatigue behavior of amorphous carbon coatings through cyclic nanoindentation

T Weikert, S Wartzack, MV Baloglu, K Willner… - Surface and Coatings …, 2021 - Elsevier
Diamond-like carbon (DLC) coatings, frequently used to reduce wear and friction in machine
components as well as on forming tools, are often subjected to cyclic loading. Doping of …

Deformation mechanisms of TiN multilayer coatings alternated by ductile or stiff interlayers

ZH Xie, M Hoffman, P Munroe, A Bendavid, PJ Martin - Acta Materialia, 2008 - Elsevier
TiN multilayers that alternate with either titanium (ductile) or nanocomposite TiSiN (hard)
interlayers were surface coated by filtered arc deposition onto stainless steel substrates …

Investigation of fracture properties of magnetron-sputtered TiN films by means of a FIB-based cantilever bending technique

S Massl, W Thomma, J Keckes, R Pippan - Acta materialia, 2009 - Elsevier
A cantilever bending technique for the determination of mode I fracture toughness and
strength of thin films is presented. First, the depth profile of residual stresses in the film is …

Erosion resistant titanium based PVD coatings on CFRP

C Maurer, U Schulz - Wear, 2013 - Elsevier
Carbon fibre reinforced plastics (CFRPs) are intensively used in aerospace applications due
to their good strength to weight ratio. However, when subjected to solid particle erosion …

Contact fatigue behavior of PVD-coated hardmetals

E Tarrés, G Ramírez, Y Gaillard… - International Journal of …, 2009 - Elsevier
There is an increasing usage of PVD-coated hardmetals in applications where contact loads
of cyclic nature between curved surfaces are common, eg cold forming tools and machine …

Contact damage and fracture micromechanisms of multilayered TiN/CrN coatings at micro-and nano-length scales

JJ Roa, E Jiménez-Piqué, R Martínez, G Ramírez… - Thin Solid Films, 2014 - Elsevier
In this study, systematic nanomechanical and micromechanical studies have been
conducted in three multilayer TiN/CrN systems with different bilayer periods (8, 19 and 25 …