Effect and mechanism of out-of-plane constraint on creep crack growth behavior of a Cr–Mo–V steel
The effect and mechanism of out-of-plane constraint on creep crack growth rates were
experimentally investigated. The results show that the out-of-plane constraint effect on creep …
experimentally investigated. The results show that the out-of-plane constraint effect on creep …
Effects of specimen geometry and loading mode on crack growth resistance curves of a high-strength pipeline girth weld
LLS Mathias, DFB Sarzosa, C Ruggieri - International Journal of Pressure …, 2013 - Elsevier
This work presents an investigation of the ductile tearing properties for a girth weld made of
an API 5L X80 pipeline steel using experimentally measured crack growth resistance …
an API 5L X80 pipeline steel using experimentally measured crack growth resistance …
Creep crack growth rate predictions in 316H steel using stress dependent creep ductility
A Mehmanparast, CM Davies, GA Webster… - Materials at High …, 2014 - Taylor & Francis
Short and long term trends in creep crack growth (CCG) rate data over test times of 500–30
000 h are available for Austenitic Type 316H stainless steel at 550° C using compact …
000 h are available for Austenitic Type 316H stainless steel at 550° C using compact …
Creep failure simulations of 316H at 550 C: Part II–Effects of specimen geometry and loading mode
In this paper, the FE damage analysis method, proposed in Part I, is applied to simulate
creep crack growth in six different types of cracked specimens of 316H at 550° C …
creep crack growth in six different types of cracked specimens of 316H at 550° C …
Crack growth in the through-thickness direction of hydrided thin-wall Zircaloy sheet
PA Raynaud, DA Koss, AT Motta - Journal of nuclear materials, 2012 - Elsevier
In a reactivity-initiated accident, cladding failure may occur by crack initiation within a defect
such as a hydride rim or blister and subsequent crack propagation through the thickness of …
such as a hydride rim or blister and subsequent crack propagation through the thickness of …
Effects of plastic pre-straining level on the creep deformation, crack initiation and growth behaviour of 316H stainless steel
A Mehmanparast, CM Davies, DW Dean… - International journal of …, 2016 - Elsevier
The effects of the material pre-straining level, in the form of plastic pre-compression at room
temperature, on the tensile, creep deformation, creep crack initiation and growth behaviour …
temperature, on the tensile, creep deformation, creep crack initiation and growth behaviour …
Creep crack growth simulations in 316H stainless steel
Virtual methods of predicting creep crack growth (CCG), using finite element analysis (FE),
are implemented in a compact tension specimen, C (T). The material examined is an …
are implemented in a compact tension specimen, C (T). The material examined is an …
In-plane and out-of-plane unified constraint-dependent creep crack growth rate of 316H steel
The unified characterization parameter A c of in-plane and out-of-plane creep constraints
along three-dimensional crack front in different specimen geometries has been analyzed …
along three-dimensional crack front in different specimen geometries has been analyzed …
[PDF][PDF] Analysis of creep crack initiation and growth in different geometries for 316H and carbon manganese steels
Results obtained from a European collaborative project aimed at producing a draft code of
practice for creep crack growth testing are presented. The tests were performed on an …
practice for creep crack growth testing are presented. The tests were performed on an …
The influence of test duration and geometry on the creep crack initiation and growth behaviour of 316H steel
Short-term creep crack growth (CCG) tests have often been performed so that they may be
incorporated into research projects with a relatively narrow time frame. Therefore tests are …
incorporated into research projects with a relatively narrow time frame. Therefore tests are …