Effect of low partial hydrogen in a mixture with methane on the mechanical properties of X70 pipeline steel

TT Nguyen, J Park, WS Kim, SH Nahm… - International journal of …, 2020 - Elsevier
In this study, the effect of a low partial hydrogen in a mixture with natural gas on the tensile,
notched tensile properties, and fracture toughness of pipeline steel X70 is investigated. An …

Hydrogen diffusivity and tensile-ductility loss of solution-treated austenitic stainless steels with external and internal hydrogen

J Yamabe, O Takakuwa, H Matsunaga, H Itoga… - International Journal of …, 2017 - Elsevier
The effects of external and internal hydrogen on the slow-strain-rate tensile (SSRT)
properties at room temperature were studied for ten types of solution-treated austenitic …

Criteria for determining hydrogen compatibility and the mechanisms for hydrogen-assisted, surface crack growth in austenitic stainless steels

S Matsuoka, J Yamabe, H Matsunaga - Engineering Fracture Mechanics, 2016 - Elsevier
To establish novel criteria for determining the hydrogen compatibility of austenitic stainless
steels, as well as to elucidate the mechanisms for hydrogen-assisted surface crack growth …

A comprehensive review of the leak flow through micro-cracks (in LBB) for nuclear system: morphologies and thermal-hydraulic characteristics

J Zhang, MJ Wang, Z Zhang, H Sun, YW Wu… - … Engineering and Design, 2020 - Elsevier
Piping cracks are widely spread in the nuclear system, which affects the safety and economy
of reactors. The leak before break (LBB) concept detects the leakage through cracks and …

Comprehensive understanding of ductility loss mechanisms in various steels with external and internal hydrogen

O Takakuwa, J Yamabe, H Matsunaga… - … Materials Transactions A, 2017 - Springer
Hydrogen-induced ductility loss and related fracture morphologies are comprehensively
discussed in consideration of the hydrogen distribution in a specimen with external and …

Effects of Cr, Mn, and Fe on the hydrogen solubility of Ni in high-pressure hydrogen environments and their electronic origins: An experimental and first-principles …

K Ito, M Yamamura, T Omura, J Yamabe… - International Journal of …, 2024 - Elsevier
Abstract Effect of the addition of Cr, Mn, or Fe to Ni on the material's hydrogen solubility are
investigated to establish guidelines for designing materials authorized to use in high …

[HTML][HTML] Transition mechanism of cycle-to time-dependent acceleration of fatigue crack-growth in 0.4% C Cr-Mo steel in a pressurized gaseous hydrogen environment

A Setoyama, Y Ogawa, M Nakamura, Y Tanaka… - International Journal of …, 2022 - Elsevier
Fatigue crack-growth (FCG) tests were conducted in 90-MPa-hydrogen gas on three
martensitic steels with tensile strengths of 811, 921 and 1025 MPa. Increased strength levels …

Hydrogen trapping and fatigue crack growth property of low-carbon steel in hydrogen-gas environment

J Yamabe, M Yoshikawa, H Matsunaga… - International Journal of …, 2017 - Elsevier
Fatigue crack growth (FCG) tests for compact-tension specimens of low-carbon steel were
performed under various combinations of hydrogen pressures (0.1–90 MPa), test …

Fatigue limit of carbon and CrMo steels as a small fatigue crack threshold in high-pressure hydrogen gas

Y Ogawa, H Matsunaga, J Yamabe… - International Journal of …, 2018 - Elsevier
The fatigue limit properties of a carbon steel and a low-alloy Crsingle bondMo steel were
investigated via fully-reversed tension-compression tests, using smooth specimens in air …

A comprehensive review on the performance analysis of composite overwrapped pressure vessels.

DS Chand - Engineering & Applied Science Research, 2022 - search.ebscohost.com
In recent decades due to the emerging use of composites, earlier metallic vessels have