Effects of direct aging on near-alpha Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM)
This study reported for the first time the selective laser melting of Ti–6Al–2Sn–4Zr–2Mo (Ti-
6242), a near-α titanium alloy specifically designed for high-temperature services. The …
6242), a near-α titanium alloy specifically designed for high-temperature services. The …
[HTML][HTML] Slip activity during low-stress cold creep deformation in a near-α titanium alloy
Near-α titanium alloys are known to be susceptible to cold dwell fatigue (CDF) debit, which
has been linked to the occurrence of cold creep during high-load dwell times superimposed …
has been linked to the occurrence of cold creep during high-load dwell times superimposed …
The influence of Zr content on microstructure and precipitation of silicide in as-cast near α titanium alloys
B Fu, H Wang, C Zou, Z Wei - Materials Characterization, 2015 - Elsevier
The influence of Zr content on microstructure and precipitation of silicide in as-cast Ti-1100-
xZr (x= 4, 6 wt.%) alloys was systematically investigated. The results demonstrate that the …
xZr (x= 4, 6 wt.%) alloys was systematically investigated. The results demonstrate that the …
Tensile and fatigue behavior of electron beam welded dissimilar joints of Ti–6Al–4V and IMI834 titanium alloys
The aim of this study was to evaluate the microstructure, hardness, tensile and fatigue
properties of electron beam welded dissimilar joints between Ti–6Al–4V and IMI834 (Ti–6Al …
properties of electron beam welded dissimilar joints between Ti–6Al–4V and IMI834 (Ti–6Al …
Investigation of crack initiation mechanism of a precipitation hardened TC11 titanium alloy under very high cycle fatigue loading
T Gao, H Xue, Z Sun, D Retraint - Materials Science and Engineering: A, 2020 - Elsevier
TC11 alpha-beta titanium alloy (Ti-6.5 Al-3.5 Mo-1.5 Zr-0.3 Si) is widely used in the
construction of aero-engine components. In service, these components are subjected to …
construction of aero-engine components. In service, these components are subjected to …
[HTML][HTML] Element segregation and α2 formation in primary α of a near-α Ti-alloy
Alloy TIMETAL® 834 is a near-α Ti-alloy typically processed to have a complex bimodal
microstructure that provides a good combination of mechanical properties at temperatures in …
microstructure that provides a good combination of mechanical properties at temperatures in …
Tensile and fatigue properties of electron beam welded dissimilar joints between Ti–6Al–4V and BT9 titanium alloys
SQ Wang, JH Liu, DL Chen - Materials Science and Engineering: A, 2013 - Elsevier
The microstructure, hardness, tensile and fatigue properties of electron beam welded
dissimilar joints between Ti–6Al–4V and BT9 (Ti–6.5 Al–3.5 Mo–1.5 Zr–0.3 Si) titanium …
dissimilar joints between Ti–6Al–4V and BT9 (Ti–6.5 Al–3.5 Mo–1.5 Zr–0.3 Si) titanium …
Superior tensile strength and microstructure evolution of TiB whisker reinforced Ti60 composites with network architecture after β extrusion
B Wang, LJ Huang, HT Hu, BX Liu, L Geng - Materials Characterization, 2015 - Elsevier
The tensile properties (at room and high temperatures) and microstructure evolution after
extrusion (1200° C) have been systematically investigated in TiBw/Ti60 composites with …
extrusion (1200° C) have been systematically investigated in TiBw/Ti60 composites with …
Strain-controlled fatigue properties of dissimilar welded joints between Ti–6Al–4V and Ti17 alloys
SQ Wang, JH Liu, DL Chen - Materials & Design, 2013 - Elsevier
The aim of this study was to evaluate the microstructure, hardness and cyclic deformation
behavior of electron beam welded dissimilar joints of Ti–6Al–4V and Ti17 (Ti–5Al–4Mo–4Cr …
behavior of electron beam welded dissimilar joints of Ti–6Al–4V and Ti17 (Ti–5Al–4Mo–4Cr …
Micromechanisms of crack initiation of a Ti-8Al-1Mo-1V alloy in the very high cycle fatigue regime
T Gao, H Xue, Z Sun, D Retraint, Y He - International Journal of Fatigue, 2021 - Elsevier
Fatigue behavior and damage mechanisms of a Ti-8Al-1Mo-1V alloy were investigated in
the very high cycle fatigue (VHCF) regime. Fracture surfaces and slip morphologies of failed …
the very high cycle fatigue (VHCF) regime. Fracture surfaces and slip morphologies of failed …