Three-layered SS321/AA1050/AA5083 explosive welds: Effect of PWHT on the interface evolution and its mechanical strength
H Pouraliakbar, G Khalaj, MR Jandaghi… - International Journal of …, 2020 - Elsevier
In this study, the effect of post-weld heat-treatment (PWHT) on the interface microstructure
and its mechanical properties in the three-layered explosive welded (EXWed) …
and its mechanical properties in the three-layered explosive welded (EXWed) …
Multilayer Cu/Al/Cu explosive welded joints: Characterizing heat treatment effect on the interface microstructure and mechanical properties
MKG Shiran, G Khalaj, H Pouraliakbar… - Journal of manufacturing …, 2018 - Elsevier
In the current research, microstructure evolution and mechanical properties of multilayer
Cu/Al/Cu explosive welded joints were studied at upper and lower interfaces after heat …
Cu/Al/Cu explosive welded joints were studied at upper and lower interfaces after heat …
Effects of heat treatment on the intermetallic compounds and mechanical properties of the stainless steel 321–aluminum 1230 explosive-welding interface
MKG Shiran, G Khalaj, H Pouraliakbar… - International Journal of …, 2017 - Springer
The effects of heat treatment on the microstructure and mechanical properties of intermetallic
compounds in the interface of stainless steel 321 explosively bonded to aluminum 1230 …
compounds in the interface of stainless steel 321 explosively bonded to aluminum 1230 …
[PDF][PDF] Effect of postweld heat treatment on interface microstructure and metallurgical properties of explosively welded bronze–carbon steel
KGM Reza, A Khoshakhlagh, G Khalaj… - J. Cent. South …, 2018 - researchgate.net
The effects of postweld heat treatment on the microstructure and metallurgical properties of a
bronze–carbon steel (st37) explosively bonded interface were studied. Explosive welding …
bronze–carbon steel (st37) explosively bonded interface were studied. Explosive welding …
Effect of stand-off distance on the mechanical and metallurgical properties of explosively bonded 321 austenitic stainless steel-1230 aluminum alloy tubes
MRKG Shiran, H Bakhtiari, SAAA Mousavi… - Materials …, 2017 - SciELO Brasil
In this research, the effect of stand-off distance on the interfacial mechanical and
metallurgical properties of explosively bonded 321 austenitic stainless steel to 1230 …
metallurgical properties of explosively bonded 321 austenitic stainless steel to 1230 …
The influence of the post-weld heat treatment on the microstructure of inconel 625/carbon steel bimetal joint obtained by explosive welding
Inconel 625 and steel P355NH were bonded by explosive welding in this study. Explosively
welded bimetal clad-plate was subjected to the two separated post-weld heat treatment …
welded bimetal clad-plate was subjected to the two separated post-weld heat treatment …
Investigation of microstructure and mechanical properties of St37 steel-Ck60 steel joints by explosive cladding
M Yazdani, MR Toroghinejad, SM Hashemi - Journal of Materials …, 2015 - Springer
The present work aimed at studying the microstructure and mechanical properties of
Ck60/St37 composite plates fabricated by explosive cladding. The explosive ratio and stand …
Ck60/St37 composite plates fabricated by explosive cladding. The explosive ratio and stand …
Comparison of microstructure and mechanical properties of titanium/steel composite plates by two manufacturing processes
X Yang, C Shi, Y Ge, MNH Sabuj - Journal of Iron and Steel Research …, 2018 - Springer
Two types of titanium/steel composite plates with the same thickness were manufactured by
parallel explosive welding and double vertical explosive welding and rolling, respectively …
parallel explosive welding and double vertical explosive welding and rolling, respectively …
Effect of post-weld heat treatment on microstructure and mechanical properties of induction pressure welded joint for A283GRC steel and 5052 aluminum alloy
K Gao, K Ye, J Gong, X Dai, H Gu, X Lei - Materials Today Communications, 2023 - Elsevier
To further enhance the mechanical characteristics of the induction pressure welding (IPW)
joint, the heat treatment was carried out for the IPW joint of A283GRC steel and 5052 …
joint, the heat treatment was carried out for the IPW joint of A283GRC steel and 5052 …
On the disintegration of A1050/Ni201 explosively welded clads induced by long-term annealing
The paper presents the microstructure and phase composition of the interface zone formed
in the explosive welding process between technically pure aluminum and nickel. Low and …
in the explosive welding process between technically pure aluminum and nickel. Low and …