The effect of Sn addition on Zn-Al-Mg alloy; Part I: Microstructure and phase composition
P Gogola, Z Gabalcová, M Kusý, H Suchánek - Materials, 2021 - mdpi.com
In this study, the addition of Sn on the microstructure of Zn 1.6 wt.% Al 1.6 wt.% Mg alloy was
studied. Currently, the addition of Sn into Zn-Al-Mg based systems has not been investigated …
studied. Currently, the addition of Sn into Zn-Al-Mg based systems has not been investigated …
[HTML][HTML] Microstructure-properties relation of hydrostatically extruded absorbable zinc alloys: Effect of Mg and Cu addition on corrosion properties and biocompatibility
A Jarzębska, M Gieleciak, A Bigos, Ł Maj… - Journal of Materials …, 2024 - Elsevier
Pure Zn is well-known for its appropriate corrosion rate, making it suitable for use as future
absorbable implants. Yet, it suffers from insufficient strength, thus, both plastic deformation …
absorbable implants. Yet, it suffers from insufficient strength, thus, both plastic deformation …
The effect of sn addition on zn-al-mg alloy; part ii: Corrosion behaviour
Z Gabalcová, P Gogola, M Kusý, H Suchánek - Materials, 2021 - mdpi.com
Corrosion behaviour of Sn (0.0, 0.5, 1.0, 2.0 and 3.0 wt.%)-doped Zn 1.6 wt.% Al 1.6 wt.%
Mg alloys exposed to salt spray testing was investigated. Intergranular corrosion was …
Mg alloys exposed to salt spray testing was investigated. Intergranular corrosion was …
Hypereutectic Zn–Al Alloys: Microstructural Development under Unsteady-State Solidification Conditions, Eutectic Coupled Zone and Hardness
The present study investigates the effects of Al content and solidification thermal parameters
on the microstructural development under transient heat flow conditions for two …
on the microstructural development under transient heat flow conditions for two …
Why are Zn-rich Zn–Mg nanoalloys optimal protective coatings against corrosion? A first-principles study of the initial stages of the oxidation process
P Álvarez-Zapatero, A Lebon, RHA Del Toro… - Physical Chemistry …, 2021 - pubs.rsc.org
ZnMg alloys of certain compositions in the Zn-rich side of the phase diagram are particularly
efficient, and widely used, as anticorrosive coatings, but a sound understanding of the …
efficient, and widely used, as anticorrosive coatings, but a sound understanding of the …
Solidification microstructure-dependent hydrogen generation behavior of Al–Sn and Al–Fe alloys in alkaline medium
This work deals with the development of quantitative correlations of hydrogen evolution
performance with solidification microstructural and thermal parameters in Al–1Sn, Al–2Sn, Al …
performance with solidification microstructural and thermal parameters in Al–1Sn, Al–2Sn, Al …
Biodegradable Zn− 1wt.% Mg (− 0.5 wt.% Mn) Alloys: Influence of Solidification Microstructure on Their Corrosion Behavior
The development of biodegradable Zn-based alloys for implants that effectively mimic the
functionality of native bone throughout the healing process is a multifaceted challenge; this …
functionality of native bone throughout the healing process is a multifaceted challenge; this …
Microstructural and segregation effects affecting the corrosion behavior of a high‐temperature Bi‐Ag solder alloy in dilute chloride solution
In electronic devices the solder joint is exposed not only to the air but also to moistures and
other corrosive media such as chlorine and sulfur compounds. Bi–Ag alloys meet the …
other corrosive media such as chlorine and sulfur compounds. Bi–Ag alloys meet the …