High-temperature sliding wear of metals
FH Stott - Tribology International, 2002 - Elsevier
Temperature can have a considerable effect on the extent of wear damage to metallic
components. During reciprocating sliding, under conditions where frictional heating has little …
components. During reciprocating sliding, under conditions where frictional heating has little …
Tribology in metal forming at elevated temperatures
K Dohda, C Boher, F Rezai-Aria, N Mahayotsanun - Friction, 2015 - Springer
The tribo-characteristics of metal forming at high temperatures have not yet been well
understood due to the complex nature of thermal, microstructural, interaction, and process …
understood due to the complex nature of thermal, microstructural, interaction, and process …
Corrosion and tribocorrosion behavior of equiatomic refractory medium entropy TiZr (Hf, Ta, Nb) alloys in chloride solutions
Abstract Equiatomic TiZr (Hf, Ta, Nb) medium entropy alloys (MEAs) were developed to
achieve higher corrosion resistance than pure Ti. Nb and Ta alloying can greatly improve …
achieve higher corrosion resistance than pure Ti. Nb and Ta alloying can greatly improve …
Friction and wear characteristics of TiO2 nano-additive water-based lubricant on ferritic stainless steel
The tribological behaviour of innovative TiO 2 nano-additive water-based lubricant on ferritic
stainless steel (FSS) 445 was characterised on a ball-on-disk tribometer. Non-oxidised …
stainless steel (FSS) 445 was characterised on a ball-on-disk tribometer. Non-oxidised …
Role of the friction layer in the high-temperature pin-on-disc study of a brake material
The tribological behavior of a commercial brake pad material, wear tested under dry sliding
conditions against a cast iron counterface disc with a pin-on-disc apparatus, was …
conditions against a cast iron counterface disc with a pin-on-disc apparatus, was …
Tribofilm formation and mild wear by tribo-sintering of nanometer-sized oxide particles on rubbing steel surfaces
H Kato, K Komai - Wear, 2007 - Elsevier
The present study is the first to show that the supply of nanometer-sized particles of Fe2O3,
SnO2, CuO, or Bi2O3 oxide on rubbing steel surfaces induces transition to mild wear with …
SnO2, CuO, or Bi2O3 oxide on rubbing steel surfaces induces transition to mild wear with …
Formation of a self-lubricating layer by oxidation and solid-state amorphization of nano-lamellar microstructures during dry sliding wear tests
C Yin, Y Liang, Y Liang, W Li, M Yang - Acta Materialia, 2019 - Elsevier
Dry sliding wear tests of steel disks of various compositions were performed with
consideration of the effects of microstructure, shear strain and shear strain rate using a ball …
consideration of the effects of microstructure, shear strain and shear strain rate using a ball …
Mechanisms of sliding wear of metals and alloys at elevated temperatures
Sliding wear at elevated temperature is an important material removal mechanism in large
number of engineering applications such as metal forming operation, gas turbine engines …
number of engineering applications such as metal forming operation, gas turbine engines …
Dry sliding wear behavior of borided hot-work tool steel at elevated temperatures
In the present study, the surface of AISI H13 hot-work tool steel was borided with EKabor II
powders using powder pack-boriding method. The process was carried out at 800, 900 and …
powders using powder pack-boriding method. The process was carried out at 800, 900 and …
The tribocorrosion resistance of TiN+ TiB/TC4 composite coatings and the synergistic strengthening effects of multi-level reinforcements
H Zhang, H Cui, C Man, F Liu, K Pang, G Ma, H Chen… - Corrosion …, 2023 - Elsevier
The Ti-based composite coating of TiN+ TiB/TC4 is successfully fabricated by laser cladding.
The results show that the addition of BN promotes the in-situ formation of an elliptic TiN …
The results show that the addition of BN promotes the in-situ formation of an elliptic TiN …