The fate and role of in situ formed carbon in polymer-derived ceramics

Q Wen, Z Yu, R Riedel - Progress in Materials Science, 2020 - Elsevier
Polymer-derived ceramics (PDCs) have been intensively studied for nearly 50 years due to
their unique advantages to producing ceramic fibers, coatings, foams, nanocomposites and …

Porous polymer derived ceramics

C Vakifahmetoglu, D Zeydanli, P Colombo - Materials Science and …, 2016 - Elsevier
Porous ceramics, in particular cellular ceramics with open and closed porosity, are key
enabling components in different demanding applications because of their favorable set of …

A review of the evolution of the nanostructure of SiCN and SiOC polymer derived ceramics and the impact on mechanical properties

E Barrios, L Zhai - Molecular Systems Design & Engineering, 2020 - pubs.rsc.org
Polymer-derived ceramics (PDCs) are fabricated through the controlled pyrolysis of silicon-
based polymeric precursors. Their structure, and subsequent material responses, are highly …

Highly porous macro-and micro-cellular ceramics from a polysilazane precursor

C Vakifahmetoglu, I Menapace, A Hirsch, L Biasetto… - Ceramics …, 2009 - Elsevier
Micro-and macro-cellular SiCN and SiOCN foams were produced via two different routes by
using a polysilazane preceramic polymer. In the first route, a mixture of partially cross-linked …

Reinforcement of precursor-derived Si–C–N ceramics with carbon nanotubes

Y Katsuda, P Gerstel, J Narayanan, J Bill… - Journal of the European …, 2006 - Elsevier
Nanocomposites consisting of precursor-derived Si–C–N ceramics incorporated with carbon
nanotubes (CNTs) were successfully prepared by casting of a mixture of CNTs and a liquid …

Glasses in the SiOCN system produced by pyrolysis of polycyclic silazane/siloxane networks

MA Schiavon, KJ Ciuffi, IVP Yoshida - Journal of non-crystalline solids, 2007 - Elsevier
In this work, polycyclic silazane/siloxane networks bearing SiO and SiN bonds were
synthesized, via hydrosilylation reaction, from cyclotrisilazane,[CH2CH (CH3) SiNH] 3, and …

Polymer‐Derived SiC/B4C/C Nanocomposites: Structural Evolution and Crystallization Behavior

Y Jiang, J Li, F Huang, Y Zhou… - Journal of the American …, 2014 - Wiley Online Library
Structural evolution and crystallization behavior between 600° C and 1450° C during the
preparation of bulk SiC/B 4 C/C nanocomposites by the pyrolysis of CB‐PSA preceramic …

Kinetic effect of boron on the thermal stability of Si–(B–) C–N polymer-derived ceramics

AH Tavakoli, P Gerstel, JA Golczewski, J Bill - Acta materialia, 2010 - Elsevier
The isothermal mass loss of two polymer-derived ceramics with compositions SiC1. 4N0. 9
and SiC1. 5N1. 0B0. 05 were measured as a function of time using thermal gravimetric …

Si‐(B‐) C‐N Ceramics Derived from Preceramic Polymers: Stability and Nano‐Composite Formation

H Schmidt - Soft Materials, 2007 - Taylor & Francis
Inorganic ceramic materials of the system Si‐(B‐) C‐N which are produced from preceramic
polymers by solid state thermolysis have gained much interest during the last years because …

Thermodynamic analysis of isothermal crystallization of amorphous Si-CN ceramics derived from polymer precursors

JA Golczewski - Journal of the Ceramic Society of Japan, 2006 - jstage.jst.go.jp