Review of hydrogen embrittlement in metals: hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention
Hydrogen dissolved in metals as a result of internal and external hydrogen can affect the
mechanical properties of the metals, principally through the interactions between hydrogen …
mechanical properties of the metals, principally through the interactions between hydrogen …
Physical metallurgy of medium-Mn advanced high-strength steels
Steels with medium manganese (Mn) content (3∼ 12 wt-%) have emerged as a new alloy
class and received considerable attention during the last decade. The microstructure and …
class and received considerable attention during the last decade. The microstructure and …
Prevention of hydrogen embrittlement in steels
HKDH Bhadeshia - ISIJ international, 2016 - jstage.jst.go.jp
The essential facts about the nature of the hydrogen embrittlement of steels have now been
known for 140 years. It is diffusible hydrogen that is harmful to the toughness of iron. It …
known for 140 years. It is diffusible hydrogen that is harmful to the toughness of iron. It …
Sustainability through alloy design: Challenges and opportunities
Exciting metallurgical breakthroughs of the last decades alongside the development and
wide-ranging availability of new and more capable experimental and theoretical tools for …
wide-ranging availability of new and more capable experimental and theoretical tools for …
Current challenges and opportunities toward understanding hydrogen embrittlement mechanisms in advanced high-strength steels: a review
Hydrogen embrittlement (HE) is one of the most dangerous yet most elusive embrittlement
problems in metallic materials. Advanced high-strength steels (AHSS) are particularly prone …
problems in metallic materials. Advanced high-strength steels (AHSS) are particularly prone …
Damage in metal forming
Physical mechanisms of ductile damage in metal forming, experimental characterization
methods for damage, and models predicting the damage level in formed components are …
methods for damage, and models predicting the damage level in formed components are …
A review of hydrogen embrittlement of martensitic advanced high-strength steels
The martensitic advanced high-strength steels (MS-AHSS) are used to create fuel-efficient,
crashworthy cars. Hydrogen embrittlement (HE) is an issue with high-strength steels; thus …
crashworthy cars. Hydrogen embrittlement (HE) is an issue with high-strength steels; thus …
The mechanism of hydrogen embrittlement in intercritically annealed medium Mn TRIP steel
J Han, JH Nam, YK Lee - Acta Materialia, 2016 - Elsevier
The objective of this study was to investigate the mechanisms of hydrogen embrittlement
(HE) in intercritically annealed medium Mn steel. For this purpose, both hot-rolled and cold …
(HE) in intercritically annealed medium Mn steel. For this purpose, both hot-rolled and cold …
Pre-strain and hydrogen charging effect on the plastic and fracture behavior of quenching and partitioning (Q&P) steel
This study investigates the fracture behavior of plastically deformed quenching and
partitioning (Q&P) steel under hydrogen conditions. The experimental results from slow …
partitioning (Q&P) steel under hydrogen conditions. The experimental results from slow …
[HTML][HTML] Mitigating hydrogen embrittlement via film-like retained austenite in 2 GPa direct-quenched and partitioned martensitic steels
Advanced (ultra) high-strength steels that utilise bcc-fcc microstructures are appealing
solutions for producing a combination of high strength and deformability. However, they are …