Microstructure evolution and mechanical responses of Al–Zn–Mg–Cu alloys during hot deformation process
Y Guo, J Zhang, H Zhao - Journal of Materials Science, 2021 - Springer
Abstract Al–Zn–Mg–Cu alloys can be fabricated by a series of thermo-mechanical
processing methods (eg, hot rolling, forging and extrusion), which is able to serve in …
processing methods (eg, hot rolling, forging and extrusion), which is able to serve in …
High-temperature tensile deformation behavior and microstructure evolution of Ti55 titanium alloy
Z Liu, P Li, L Xiong, T Liu, L He - Materials Science and Engineering: A, 2017 - Elsevier
High temperature tensile and electron backscatter diffraction (EBSD) techniques were
combined to perform a systematic investigation for the hot deformation behavior and …
combined to perform a systematic investigation for the hot deformation behavior and …
Effect of retrogression treatments on microstructure, hardness and corrosion behaviors of aluminum alloy 7085
Y Wang, L Cao, X Wu, X Tong, B Liao, G Huang… - Journal of Alloys and …, 2020 - Elsevier
The microstructure, hardness and corrosion resistance of aluminum alloy 7085 after different
retrogression and re-aging (RRA) treatments were investigated. The results showed that the …
retrogression and re-aging (RRA) treatments were investigated. The results showed that the …
[HTML][HTML] Microstructure evolution mechanisms and a physically-based constitutive model for an Al–Zn–Mg–Cu–Zr aluminum alloy during hot deformation
High-temperature flow features of the Al− Zn− Mg− Cu− Zr aluminum alloy was revealed by
hot compression tests. The evolution mechanisms of dislocation clusters, subgrain, and …
hot compression tests. The evolution mechanisms of dislocation clusters, subgrain, and …
Microstructural evolution of a nickel-based superalloy during hot deformation
Hot compressive tests of a nickel-based superalloy are performed under the strain rate
range of 0.001–1 s− 1 and deformation temperature range of 920–1040° C. Optical …
range of 0.001–1 s− 1 and deformation temperature range of 920–1040° C. Optical …
Work-hardening behaviors of typical solution-treated and aged Ni-based superalloys during hot deformation
A detailed analysis of work-hardening behavior is useful to optimize the hot forming
processing of metals or alloys. The hot compression tests of solution-treated and aged Ni …
processing of metals or alloys. The hot compression tests of solution-treated and aged Ni …
Elevated temperature mechanical properties of TiCN reinforced AlSi10Mg fabricated by laser powder bed fusion additive manufacturing
This short communication presents 2–4 μm sized TiCN reinforced AlSi10Mg composites
(TiCN/AlSi10Mg) fabricated by laser powder bed fusion (LPBF) with refined Al-Si eutectic …
(TiCN/AlSi10Mg) fabricated by laser powder bed fusion (LPBF) with refined Al-Si eutectic …
Constitutive modeling for the simulation of the superplastic forming of TA15 titanium alloy
T Yasmeen, Z Shao, L Zhao, P Gao, J Lin… - International Journal of …, 2019 - Elsevier
Titanium alloy, TA15, has a high strength-to-weight ratio, high weldability, and superior
creep resistance at high temperatures up to 550° C. TA15 is difficult to deform, especially for …
creep resistance at high temperatures up to 550° C. TA15 is difficult to deform, especially for …
[HTML][HTML] Evaluation of constitutive equations for modeling and characterization of microstructure during hot deformation of sintered Al–Zn–Mg alloy
Commercial simulation software like QFORM and DEFORM do not possess adequate
material data for alloys produced through powder metallurgy. Therefore, in the present …
material data for alloys produced through powder metallurgy. Therefore, in the present …
[HTML][HTML] Microstructural and constitutive relationship in process modeling of hot working: The case of a 60Mg-30Pb-9.2 Al-0.8 B magnesium alloy
B Li, Y Duan, S Zheng, M Peng, M Li, H Bu - Journal of Materials Research …, 2023 - Elsevier
Hot compression tests in the temperature range of 493-653 K and strain rates of 0.01-10.00
s− 1 were used to evaluate the hot deformation behavior of 60Mg-30Pb-9.2 Al-0.8 B alloy. In …
s− 1 were used to evaluate the hot deformation behavior of 60Mg-30Pb-9.2 Al-0.8 B alloy. In …