Mechanism of corrosion protection in chloride solution by an apple-based green inhibitor: experimental and theoretical studies

M Honarvar Nazari, MS Shihab, EA Havens… - Journal of infrastructure …, 2020 - Springer
Preservation of metals in infrastructures and other assets requires cost-effective and
sustainable solutions such as green corrosion inhibitors. This study assesses an apple …

A peony-leaves-derived liquid corrosion inhibitor: protecting carbon steel from NaCl

M Honarvar Nazari, MS Shihab, L Cao… - … Chemistry Letters and …, 2017 - Taylor & Francis
ABSTRACT A liquid mixture was developed from waste peony leaves through a zero-waste
chemical/biological process. The inhibition effect of different concentrations of peony leaves …

Characterization and corrosion behavior of electroless Ni–P/nano-SiC coating inside the CO2 containing media in the presence of acetic acid

SR Allahkaram, MH Nazari, S Mamaghani… - Materials & Design, 2011 - Elsevier
In this research, Ni–P and Ni–P/nano-SiC coatings were applied on the X70 steel substrate
successfully without any surfactant. Then, CO2 corrosion in the presence of acetic acid …

Effect of free Cr content on corrosion behavior of 3Cr steels in a CO2 environment

W Li, L Xu, L Qiao, J Li - Applied Surface Science, 2017 - Elsevier
The corrosion behavior of 3Cr steels with three microstructures (martensite, bainite,
combined ferrite and pearlite) in simulated oil field formation water with a CO 2 partial …

[HTML][HTML] Benchmarking the impact of nickel filler addition, weld hardness, environmental pH, and corrosion inhibitors on A333 carbon steel pipe weld corrosion

NMRNM Daud, KK Eng, K Jumbri, AM Nor… - Results in …, 2023 - Elsevier
This study addresses the challenge of preferential weld corrosion in ASTM A333 carbon
steel piping, investigating the intricate interplay of various factors. The welding process …

Performance enhancement of zero valent iron based systems using depassivators: Optimization and kinetic mechanisms

KVK Ansaf, S Ambika, IM Nambi - Water Research, 2016 - Elsevier
The long-term ability of Zero-Valent Iron (ZVI) in contaminant removal relies on the
effectiveness of iron to serve as electron donor, which makes it a versatile remediation …

Crevice corrosion of N80 carbon steel in CO2-saturated environment containing acetic acid

YZ Li, N Xu, GR Liu, XP Guo, GA Zhang - Corrosion Science, 2016 - Elsevier
Crevice corrosion of N80 carbon steel in CO 2-saturated environment containing acetic acid
(HAc) was studied by electrochemical measurements and surface analysis. No obvious …

Enhancing degradation and corrosion resistance of AZ31 magnesium alloy through hydrophobic coating

C Hsu, MH Nazari, Q Li, X Shi - Materials chemistry and physics, 2019 - Elsevier
AZ31 magnesium alloy is a promising implant metallic material for the process of healing
hard tissue in the human body. However, it is susceptible to degradation when exposed to …

Synergistic effect of stress and crevice on the corrosion of N80 carbon steel in the CO2-saturated NaCl solution containing acetic acid

YZ Li, XP Guo, GA Zhang - Corrosion Science, 2017 - Elsevier
The corrosion behaviour of N80 carbon steel under the coexistence of stress and crevice in
the CO 2-saturated NaCl solution containing acetic acid (HAc) was studied by …

An investigation on electroless Cu–P composite coatings with micro and nano-SiC particles

S Faraji, AH Faraji, SR Noori - Materials & Design (1980-2015), 2014 - Elsevier
Cu–P/micro-SiC and Cu–P/nano-SiC composite coatings were deposited by electroless