Effect of Al alloys on selective laser melting behaviour and microstructure of in situ formed particle reinforced composites
S Dadbakhsh, L Hao - Journal of alloys and compounds, 2012 - Elsevier
This work investigates the effects of various Al alloys (including Al, AlMg1SiCu, and
AlSi10Mg), mixed with 15wt% Fe2O3, on the selective laser melting (SLM) facilitated in situ …
AlSi10Mg), mixed with 15wt% Fe2O3, on the selective laser melting (SLM) facilitated in situ …
[HTML][HTML] Investigation of a novel functionally graded material for the repair of premium hypereutectoid rails using laser cladding technology
Q Lai, R Abrahams, W Yan, C Qiu, P Mutton… - Composites Part B …, 2017 - Elsevier
In this study, the effects of cladding direction, preheating and post heat treatment on
microstructural and mechanical properties of laser cladded rail repairs are presented. Laser …
microstructural and mechanical properties of laser cladded rail repairs are presented. Laser …
Sb effect on micro structural and mechanical properties of rapidly solidified Al–12Si alloy
The effects of antimony (Sb) addition on the microstructure and mechanical properties of
rapidly solidified eutectic Al–Si alloy were investigated. Al–12wt.% Si–Xwt.% Sb (X= 0, 0.5 …
rapidly solidified eutectic Al–Si alloy were investigated. Al–12wt.% Si–Xwt.% Sb (X= 0, 0.5 …
Diamond tool wear during ultra-high precision machining of rapidly solidified aluminium RSA 905
K Abou-El-Hossein, O Olufayo, Z Mkoko - Wear, 2013 - Elsevier
Aluminium alloys such as AA 6061-T6 are used to create forming optical surfaces in mould
cavities for the injection of plastic optical components. However, 6061-T6 aluminium is …
cavities for the injection of plastic optical components. However, 6061-T6 aluminium is …
Structure and properties of nanostructured Cu-13.2 Al-5.1 Ni shape memory alloy produced by melt spinning
M Izadinia, K Dehghani - Transactions of Nonferrous Metals Society of …, 2011 - Elsevier
The microstructure and properties of nanostructured Cu-13.2 Al-5.1 Ni shape memory alloy
(SMA) were compared with those of initial coarse structure. The nanostructured Cu-Al-Ni …
(SMA) were compared with those of initial coarse structure. The nanostructured Cu-Al-Ni …
Effects of Sr, Ce and P on the microstructure and mechanical properties of rapidly solidified Al7Si alloys
A series of Alsingle bond 7Si based alloys with trace addition of Sr, Ce or P were prepared
using melt-spinning at two different high cooling rates, and the microstructure as well as the …
using melt-spinning at two different high cooling rates, and the microstructure as well as the …
The enhanced microhardness in a rapidly solidified Al alloy
Y Lin, S Mao, Z Yan, Y Zhang, L Wang - Materials Science and …, 2017 - Elsevier
The objective of the present study is to explore the feasibility of producing 7075 Al alloy
ribbons with the increased microhardness via rapid solidification processing, namely melt …
ribbons with the increased microhardness via rapid solidification processing, namely melt …
Nanostructure evolution, thermal stability and hardness of amorphous Al–Cu-Y (Co, La)(at.%) alloys
M Salehi, SG Shabestari - Journal of Non-Crystalline Solids, 2022 - Elsevier
Al alloys with nominal composition of Al 86 Cu 6 Y 6 Co 2, Al 86 Cu 6 Y 6 La 2 and Al 84 Cu
6 Co 2 Y 6 La 2 (at.%) were studied in as-spun and annealed states using differential …
6 Co 2 Y 6 La 2 (at.%) were studied in as-spun and annealed states using differential …
Structure and properties of nanostructured A357 alloy produced by melt spinning compared with direct chill ingot
Z Chen, Y Lei, H Zhang - Journal of alloys and compounds, 2011 - Elsevier
The properties of nanostructured A357 ribbons produced by melt spinning were investigated
using field emission gun scanning electron microscope, X-ray diffraction pattern, differential …
using field emission gun scanning electron microscope, X-ray diffraction pattern, differential …
Formation of nanostructured weldments in the Al–Si system using electrospark welding
Electrospark welding (ESW) electrodes were manufactured from three binary aluminum–
silicon alloys consisting of 12 and 17wt% silicon, produced using chill and sand casting. The …
silicon alloys consisting of 12 and 17wt% silicon, produced using chill and sand casting. The …